PA6 Zytel® 73G45L DUPONT USA
84
- Unit Price:
- $3718 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Thermal stability Filler: Glass fiber reinf 45% filler by weight
- Application Areas:Electronic and electrical Automotive Applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Moisture Absorption | Saturation,23°C,2.00mm | ISO62 | 4.9 | % |
Equilibrium,23°C,2.00mm,50%RH | ISO62 | 1.5 | % | |
Modeling Shrinkage | TD | ISO294-4 | 0.90 | % |
MD | ISO294-4 | 0.10 | % | |
Density / Specific Gravity | ISO1183 | 1.51 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Creep Modulus | 1000hr | ISO899-1 | -- | Mpa |
Tensile Creep Modulus | 1hr | ISO899-1 | -- | Mpa |
Tensile Stress | Break | ISO527-2 | 230 | Mpa |
Tensile Strain | Break | ISO527-2 | 3.0 | % |
Tensile Modulus | ISO527-2 | 14500 | Mpa | |
Flexural Modulus | ISO178 | 13000 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 221 | °C |
1.8MPa,Unannealed | ISO75-2/A | 213 | °C | |
Vicat Softening Temperature | ISO306/B50 | 215 | °C | |
Linear thermal expansion coefficient | MD | ISO11359-2 | 1.6E-05 | cm/cm/°C |
TD | ISO11359-2 | 1E-04 | cm/cm/°C | |
Melting Temperature | ISO11357-3 | 221 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | 120 | kJ/m² |
23°C | ISO179/1eU | 120 | kJ/m² | |
Charpy Notched Impact Strength | -30°C | ISO179/1eA | 19 | kJ/m² |
23°C | ISO179/1eA | 20 | kJ/m² | |
Notched Izod Impact Strength | -30°C | ISO180/1A | 15 | kJ/m² |
23°C | ISO180/1A | 18 | kJ/m² |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 1.5mm | UL94 | HB | |
FMVSS Flammability | FMVSS302 | B | ||
Burning Rate | 1.00mm | ISO3795 | 44 | mm/min |
Flammability level | 1.5mm | IEC60695-11-10,-20 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.