PA6 Ultramid® B3WG6 BK BASF MALAYSIA
79
- Unit Price:
- $2903 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 44.2MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Thermal stability Oil resistant Filler: Glass fiber reinf 30% Filler by weight 30% filler by weight
- Application Areas:Engine hood parts Automotive sector Application in the automo
- Color:--
- Grade:Enhanced level
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.18mm | 0.30 | % | |
Moisture Absorption | Saturation | ASTMD570 | 6.6 | % |
Saturation,23°C | ISO62 | 6.6 | % | |
Equilibrium,50%RH | ASTMD570 | 2.1 | % | |
Equilibrium,23°C,50%RH | ISO62 | 2.1 | % | |
Melt Volume flow Rate | 275°C/5.0kg | ISO1133 | 40.0 | cm3/10min |
Density / Specific Gravity | ASTMD792 | 1.36 | g/cm³ | |
ISO1183 | 1.36 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Modulus | 23°C | ISO527-2 | 9500 | Mpa |
Flexural Modulus | 23°C | ISO178 | 8300 | Mpa |
Tensile Stress | Break,23°C | ISO527-2 | 180 | Mpa |
Tensile Strain | Break,23°C | ISO527-2 | 3.0 | % |
Tensile Strength | Break,23°C | ASTMD638 | 180 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Peak Melting Temperature | ASTMD3418 | 220 | °C | |
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ASTMD648 | 220 | °C |
0.45MPa,Unannealed | ISO75-2/B | 220 | °C | |
1.8MPa,Unannealed | ASTMD648 | 210 | °C | |
1.8MPa,Unannealed | ISO75-2/A | 205 | °C | |
Melting temperature (DSC) | ISO3146 | 220 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | -30°C | ISO179 | 9.0 | kJ/m² |
23°C | ISO179 | 12 | kJ/m² | |
Notched Izod Impact Strength | -40°C | ASTMD256 | 110 | J/m |
23°C | ASTMD256 | 150 | J/m | |
23°C | ISO180 | 12 | kJ/m² | |
Charpy Unnotched Impact Strength | -30°C | ISO179 | 65 | kJ/m² |
23°C | ISO179 | 80 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.