Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melt Mass-Flow Rate | 230°C/2.16 kg | ISO 1133 | 12 | g/10 min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Modulus | | ISO 527-1/1 | 1550 | Mpa |
Tensile Strain | Yield | | 8 | % |
Tensile Strain | Break | | > 50 | % |
Tensile Stress | Yield | ISO 527-2/50 | 35 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load (0.45Mpa Unannealed) | | ISO 75-2/B | 85 | °C |
Injection | Test Condition | Test Method | Test Result | Unit |
---|
Processing (Melt) Temp | | | 220 到 260 | °C |
Mold Temperature | | | 20 到 40 | °C |
Holding Pressure | | | 20.0 到 50.0 | Mpa |
Injection Rate | | | 快速 | |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Notched Izod Impact Strength | 23°C | ISO 180/1A | 3 | kJ/m² |
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 3 | kJ/m² |
Charpy Unnotched Impact Strength | | ISO 179/1eU | 110 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.