Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melt index | | Q/SHPRD255-2009(2012) | 19.8 | g/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Stress(Yield) | | Q/SH PRD255-2009(2012) | 32.7 | Mpa |
Flexural Modulus | | Q/SH PRD255-2009(2012) | 1294 | Mpa |
Charpy Notched Impact Strength | 23℃ | Q/SH PRD255-2009(2012) | 2.0 | kJ/m² |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | Tf0.45 | Q/SH PRD255-2009(2012) | 77.7 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Powder Ash Content | 质量分数 | Q/SH PRD255-2009(2012) | 0.015 | % |
Other performance | Test Condition | Test Method | Test Result | Unit |
---|
Haze | | GB/T 2410-2008 | 12.4 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.