Material Description
Technical Data Sheet
Material Description
- Material Properties:heat-resisting transparent High mobility
- Application Areas:packing Kitchen utensils Electrical/Electronic App Electrical appliances Household fan blades container small home appliances
- Color:--
- Grade:Chemical resistance
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.20mm | ASTMD955 | 0.40to0.70 | % |
Moisture Absorption | Saturation | ISO622 | 0.16 | % |
Melt Mass-Flow Rate | 200°C/5.0kg | ASTMD1238 | 3.0 | g/10min |
220°C/10.0kg | ASTMD1238 | 29 | g/10min | |
230°C/3.8kg | ASTMD1238 | 10 | g/10min | |
Density / Specific Gravity | ASTMD792 | 1.07 | g/cm³ | |
ISO11832 | 1070 | kg/m3 | ||
Melt Mass-Flow Rate | 220°C/10.0kg | ISO11332 | 31.0 | cm3/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Strain | Break,3.20mm | ASTMD638 | 6.0 | % |
Flexural Modulus | 3.20mm | ASTMD790 | 3680 | Mpa |
Tensile Modulus | 3.20mm | ASTMD638 | 3110 | Mpa |
Tensile Strength | Yield,3.20mm | ASTMD638 | 73.5 | Mpa |
Flexural Strength | 3.20mm | ASTMD790 | 118 | Mpa |
Tensile Modulus | ISO527-22 | 3300 | Mpa | |
Tensile Stress | Break | ISO527-22 | 70.0 | Mpa |
Tensile Strain | Break | ISO527-22 | 6.0 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
RTIElec | UL746 | 50.0 | °C | |
Evolution Calendar intelligent importer | UL746 | 50.0 | °C | |
RTIStr | UL746 | 50.0 | °C | |
Linear thermal expansion coefficient | MD | ISO11359-22 | 6.7E-05 | cm/cm/°C |
TD | ISO11359-22 | 6.7E-05 | cm/cm/°C | |
Deflection Temperature Under Load? | 1.8MPa,Unannealed,6.40mm | ASTMD648 | 90.0 | °C |
Glass Transition Temperature | ISO11357-22 | 110 | °C | |
Vicat Softening Temperature | ASTMD1525 | 100 | °C | |
50N | ISO3062 | 100 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Electric strength | IEC60243-12 | 51 | KV/mm | |
Surface Resistivity | IEC600932 | >1.0E+15 | ohms | |
Volume Resistivity | IEC600932 | >1.0E+13 | ohms·m | |
Comparative Tracking Index | IEC601122 | 375 |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | -30°C | ISO179/1eA2 | 2.00 | kJ/m² |
Notched Izod Impact Strength | -30°C,6.40mm | ASTMD256 | 9.8 | J/m |
23°C,6.40mm | ASTMD256 | 9.8 | J/m | |
CharpyNotchedImpactStrength | 23°C | ISO179/1eA2 | 2.80 | kJ/m² |
Charpy impact strength | 23°C | ISO179/1eU2 | 13.0 | kJ/m² |
Charpy Notched Impact Strength | -30°C | ISO179/1eU2 | 4.80 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | R-Scale | ASTMD785 | 123 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 1.6mm | UL94 | HB | |
3.2mm | UL94 | HB | ||
Burning Behav.atthicknessh | 3.20mm,UL | ISO12102 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.