ABS POLYLAC® PA-763A TAIWAN CHIMEI
110
- Unit Price:
- $3533 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 20MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Flame retardant High impact resistance High temperature resistan
- Application Areas:Electrical field Electronic field
- Color:--
- Grade:Flame retardant grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt Mass-Flow Rate | 200°C/5.0kg | ASTMD1238 | 2.8 | g/10min |
Melt Volume flow Rate | 220°C/10.0kg | ISO1133 | 27.0 | cm3/10min |
Density / Specific Gravity | --3 | ASTMD792 | 1.19 | g/cm³ |
23°C | ISO1183 | 1.19 | g/cm³ | |
Modeling Shrinkage | ISO294-4 | 0.30到0.60 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Strength | Yield4 | ASTMD638 | 38.6 | Mpa |
Yield | ISO527-2/50 | 38.0 | Mpa | |
Break | ISO527-2/50 | 29.0 | Mpa | |
Tensile Elongation | Break4 | ASTMD638 | 30 | % |
Break | ISO527-2/50 | 15 | % | |
Flexural Modulus | --5 | ASTMD790 | 2410 | Mpa |
--6 | ISO178 | 2000 | Mpa | |
Flexural Strength | --5 | ASTMD790 | 60.7 | Mpa |
--6 | ISO178 | 58.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ASTMD648 | 85.0 | °C |
1.8MPa,Unannealed | ISO75-2/A | 86.0 | °C | |
1.8MPa,Annealed | ASTMD648,ISO75-2/A | 96.0 | °C | |
Vicat Softening Temperature | -- | ASTMD15257 | 104 | °C |
-- | ISO306/A50 | 103 | °C | |
-- | ISO306/B50 | 96.0 | °C | |
Linear thermal expansion coefficient | MD | ISO11359-2 | 8.5E-05 | cm/cm/°C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | -30°C | ISO179 | 12 | kJ/m² |
23°C | ISO179 | 22 | kJ/m² | |
Notched Izod Impact Strength | 23°C,3.20mm | ASTMD256 | 230 | J/m |
23°C,6.40mm | ASTMD256 | 200 | J/m | |
-30°C | ISO180/1A | 11 | kJ/m² | |
23°C | ISO180/1A | 21 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | R-Scale | ASTMD785 | 98 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 1.5mm | UL94 | V-0 | |
2.5mm | UL94 | 5VA |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.