ABS Toyolac® 700 BK TORAY JAPAN
113
- Unit Price:
- $1933 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High mobility
- Application Areas:Electrical appliances Electronic and Electrical
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density/specific gravity | ASTMD792 | 1.05 | g/cm³ | |
ISO1183 | 1.04 | g/cm³ | ||
Melt mass flow rate | 220°C/10.0kg | ISO1133 | 40 | g/10min |
Shrinkage rate | MD | ASTMD955 | 0.40to0.60 | % |
Water absorption rate | 23°C,24hr | ASTMD570 | 0.30 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ISO527-2/1 | 2600 | Mpa | |
Tensile strength 2 | Yield | ASTMD638 | 46.0 | Mpa |
Tensile stress | Yield | ISO527-2/50 | 51.0 | Mpa |
Elongation rate 2 | Break | ASTMD638 | 15 | % |
Tensile strain | Break | ISO527-2/50 | >10 | % |
Bending modulus 3 | ASTMD790 | 2300 | Mpa | |
Bending strength 3 | ASTMD790 | 73.0 | Mpa | |
Bending stress 4 | ISO178 | 77.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed,6.40mm | ASTMD648 | 86.0 | °C |
1.8MPa,Unannealed,12.7mm | ASTMD648 | 92.0 | °C | |
1.8MPa,Unannealed | ISO75-2/A | 81.0 | °C | |
Linear coefficient of thermal expansion | MD | ASTMD696 | 7.2E-05 | cm/cm/°C |
thermal conductivity | ASTMC177 | 0.16 | W/m/K |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistivity 5 | ASTMD257 | >1.0E+16 | ohms | |
Volume resistivity | 23°C | ASTMD257 | >1.0E+16 | ohms·cm |
Dielectric strength 6 | ASTMD149 | 23 | KV/mm | |
Dielectric constant | 1kHz | ASTMD150 | 3.10 | |
Dissipation factor | 1kHz | ASTMD150 | 6.2E-03 |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 18 | kJ/m² |
Impact strength of cantilever beam gap | -30°C,3.20mm | ASTMD256 | 110 | J/m |
-30°C,12.7mm | ASTMD256 | 80 | J/m | |
0°C,3.20mm | ASTMD256 | 160 | J/m | |
0°C,12.7mm | ASTMD256 | 110 | J/m | |
23°C,3.20mm | ASTMD256 | 220 | J/m | |
23°C,12.7mm | ASTMD256 | 200 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | R-Scale | ASTMD785 | 114 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | UL94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.