ABS Novodur® HH-106 INEOS STYRO KOREA
101
- Unit Price:
- $3529 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:heat-resisting
- Application Areas:Electronic field Application in the automo Automotive interior parts
- Color:--
- Grade:Heat resistant grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD | ASTMD955 | 0.55 | % |
ISO294-4 | 0.40to0.70 | % | ||
Moisture Absorption | Equilibrium,23°C,50%RH | ISO62 | 0.25 | % |
Melt Mass-Flow Rate | 220°C/10.0kg | ASTMD1238 | 7.0 | g/10min |
Melt Volume flow Rate | 220°C/10.0kg | ISO1133 | 7.00 | cm3/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Ball Indentation Hardness | ISO2039-1 | 102 | Mpa | |
Nominal Tensile Strain at Break | 23°C | ISO527-2 | 9.0 | % |
Tensile Stress | Yield,23°C | ISO527-2 | 51.0 | Mpa |
Tensile Strain | Yield,23°C | ISO527-2 | 3.0 | % |
Tensile Strength | Yield,23°C | ASTMD638 | 52.0 | Mpa |
Flexural Stress | ISO178 | 72.0 | Mpa | |
Tensile Modulus | ASTMD638 | 2500 | Mpa | |
ISO527-2 | 2400 | Mpa | ||
Tensile Elongation | Break | ASTMD638 | 3.0 | % |
Flexural Modulus | ASTMD790 | 2400 | Mpa | |
ISO178 | 2400 | Mpa | ||
Flexural Strength | ASTMD790 | 77.2 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Linear thermal expansion coefficient | MD | ISO11359-2 | 9E-05 | cm/cm/°C |
Vicat Softening Temperature | -- | ISO306/A50 | 115 | °C |
-- | ISO306/B50 | 106 | °C | |
Maximum Service Temperature | 85 | °C | ||
Heat Deflection Temperature | 0.45MPa,Annealed | ISO75-2/B | 107 | °C |
1.8MPa,Annealed | ISO75-2/A | 99.0 | °C | |
Thermal Conductivity | DIN52612 | 0.17 | W/m/K |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Comparative Tracking Index | IEC60112 | 600 | V | |
Electric strength | 1.50mm | IEC60243-1 | 39 | KV/mm |
Volume Resistivity | ASTMD257 | >1.0E+15 | ohms·cm | |
IEC60093 | 1E+15 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | -30°C | ISO179 | 100 | kJ/m² |
23°C | ISO179 | 190 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.