ABS Toyolac® 920 TORAY JAPAN
87
- Unit Price:
- $2501 USD/MT
- Packaging Specification:
- 25KG/PKG
- Supply Quantity:
- 58.6MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density | ASTM D792/ISO 1183 | 1.09 | ||
Melt Mass-Flow Rate | ASTM D1238/ISO 1133 | 25 | g/10min |
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt index | 220℃/10kg | ISO 1133 | 25 | g/10min |
220℃ 10kg | ASTM D-1238 | 19~23 | g/10min | |
Flammability | UL-94 | 94HB | ||
Melt Viscosity | 220℃ | 3.5~5.0 | ||
Moisture Absorption | 浸入23℃水中24hr | ASTM D-570 | 0.3 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural strength | 23℃ | ASTM D-790 | 780 | kg/cm |
Tensile Strain(Break) | 23℃ | ISO 527-2 | 17 | % |
Tensile Strength (Yield) | 23℃ | ASTM D-638 | 490 | kg/cm |
Tensile Strength (Yield) | 23℃ | ASTM D-638 | 3.5 | % |
Tensile Strength (Break) | 23℃ | ASTM D-638 | 30 | % |
Tensile Strength (Break) | 23℃ | ASTM D-790 | 23500 | kg/cm |
Tensile Strength(Break) | 23℃ | ASTM D-638 | 380 | kg/cm |
Tensile Elongation?(Break) | ASTM D638/ISO 527 | 20 | % | |
Tensile Strength | ASTM D638/ISO 527 | 48 | kg/cm²(MPa)[Lb/in²] | |
Rockwell Hardness | ASTM D785 | 115 | ||
23℃ | ASTM D-785 | 115 | R | |
Flexural Modulus | ASTM D790/ISO 178 | 2160 | kg/cm²(MPa)[Lb/in²] | |
Flexural Strength | ASTM D790/ISO 178 | 74 | kg/cm²(MPa)[Lb/in²] | |
Impact Strength | 12.7×12.7×62.5mm(带韧口),23℃;0℃;-30℃ | ASTM D-256 | 9;7;6 | kg.cm/cm |
3.2×12.7×62.5mm(带韧口),23℃;0℃;-30℃ | ASTM D-256 | 10;7;6 | kg.cm/cm | |
Tensile Stress(Yield) | 23℃ | ISO 527-2 | 54.0 | Mpa |
Izod notch impact strength | ASTM D256/ISO 179 | 108 | kg·cm/cm(J/M)ft·lb/in |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | UL 94 | HB | ||
Burning Rate | UL94 | HB | ||
Deflection Temperature Under Load? | ASTM D648/ISO 75 | 83 | ℃(℉) | |
18.56kg/cm | ASTM D-648 | 89 | °C | |
1.8MPa,Unannealed | ISO 75-2/A | 77.0 | °C | |
Linear expansion coefficient | ASTM D-696 | 1.2×10 | mm/mm/℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.