LLDPE TAISOX® 3224 FPC TAIWAN
109
- Unit Price:
- $1281 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 41MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:low density Medium smooth anticaking Strippable Heat sealing performance
- Application Areas:film Stretch winding
- Color:--
- Grade:Thin film grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt Mass-Flow Rate | 190°C/2.16kg | ASTMD1238 | 2.0 | g/10min |
Density / Specific Gravity | ASTMD1505 | 0.920 | g/cm³ |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Vicat Softening Temperature | ASTMD1525 | 93.0 | °C | |
Brittleness Temperature | ASTMD746 | -70.0 | °C | |
Melting temperature | 122 | °C |
Film | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Film Thickness - Tested) | 38 | µm | ||
Secant Modulus | 1%Secant,MD:38μm,Blown Film | ASTMD882 | 147 | Mpa |
1%Secant,TD:38μm,Blown Film | ASTMD882 | 206 | Mpa | |
Tensile Elongation | MD:Break,38μm,Blown Film | ASTMD882 | 600 | % |
TD:Break,38μm,Blown Film | ASTMD882 | 800 | % | |
Elmendorf Tear Strength | MD:38μm,Blown Film | ASTMD1922 | 61 | g |
TD:38μm,Blown Film | ASTMD1922 | 650 | g | |
Tensile Strength | MD:Yield,38μm,Blown Film | ASTMD882 | 9.81 | Mpa |
TD:Yield,38μm,Blown Film | ASTMD882 | 10.8 | Mpa | |
MD:Break,38μm,Blown Film | ASTMD882 | 35.3 | Mpa | |
TD:Break,38μm,Blown Film | ASTMD882 | 27.5 | Mpa | |
Gardner Impact | 38μm,Blown Film | ASTMD1709 | 120 | g |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Haze | 38.0μm,Blown Film | ASTMD1003 | 24 | % |
Gloss | 45°,38.0μm,Blown Film | ASTMD2457 | 47 | |
Transmittance | ASTMD1746 | 53.0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.