POM HOSTAFORM® MT12U01 CELANESE GERMANY
173
- Unit Price:
- $17898 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Antisolvent antioxidant Impact resistance Antichemical Low friction coefficient
- Application Areas:Thin walled products Electrical tools Automotive Applications
- Color:--
- Grade:Blow molding grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | TD Across Flow | ISO 294-4 | 1.8 | % |
MD Flow | ISO 294-4 | 2 | % | |
Density | ISO 1183 | 1.41 | g/cm³ | |
Melt Volume flow Rate | 190℃,2.16 kg 190℃/2.16 kg | ISO 1133 | 12 | cm3/10min |
Moisture Absorption | Saturation,23℃ Saturation,23℃ | ISO 62 | 0.65 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Strength | Yield Yield | ISO 527-2/1A/50 | 65 | Mpa |
Tensile Creep Modulus | 1000 hr 1000 hr | ISO 899-1 | 1300 | Mpa |
Nominal Tensile Strain at Break | ISO 527-2/1A/50 | 25 | % | |
Tensile Creep Modulus (1 hr) | ISO 899-1 | 2500 | Mpa | |
Flexural Modulus | 23℃ 23℃ | ISO 178 | 2800 | Mpa |
Tensile Modulus | ISO 527-2/1A/1 | 2900 | Mpa | |
Tensile Strain | Yield Yield | ISO 527-2/1A/50 | 9 | % |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | -30℃ -30°C | ISO 179/1eU | 140 | kJ/m² |
23℃ 23°C | ISO 179/1eU | 150 | kJ/m² | |
Charpy Notched Impact Strength | -30℃ -30°C | ISO 179/1eA | 6 | kJ/m² |
23℃ 23°C | ISO 179/1eA | 6 | kJ/m² |
Thermal | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Heat Deflection Temperature | 1.8 MPa,Unannealed 1.8 MPa,Unannealed | ISO 75-2/A | 106 | °C |
Coefficient of Linear Thermal Expansion | MD MD | ISO 11359-2 | 0.00011 | 1/℃ |
Melting temperature | ISO 11357-3 | 166 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.