Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | 3.2mm | ASTM D-955 | 5-7 | |
Density / Specific Gravity | | ASTM D-792 | 1.11 | |
Flame retardancy | | UL 94 | V-0 | |
Flame retardancy | | UL 94 | 0.8 | mm |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Notched Impact Strength | 23°C | ASTM D-256 | 160 | J/m |
Tensile Strength | Yield点,3.2mm | ASTM D-638 | 75 | Mpa |
Tensile Strength | Break点,3.2mm | ASTM D-638 | 18 | Mpa |
Flexural Modulus | 6.4mm | ASTM D-790 | 2646 | Mpa |
Flexural Strength | 6.4mm | ASTM D-790 | 112 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 0.45MPa | ASTM D-648 | 133 | °C |
Deflection Temperature Under Load? | 1.8MPa | ASTM D-648 | 122 | °C |
Vicat Softening Temperature | | ASTM D-1525 | 150 | °C |
UL Long-Term Service Temperature | 电气 | UL 746B | 105 | °C |
UL Long-Term Service Temperature | 含冲击 | UL 746B | 100 | °C |
UL Long-Term Service Temperature | 无冲击 | UL 746B | 105 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Surface Resistivity | | ASTM D-257 | 1.0×10 | Ω.cm |
Dielectric Constant | 1MHz | ASTM D-150 | 2.49 | |
Volume Resistivity | | ASTM D-257 | 2.0×10 | Ω.cm |
Physical | Test Condition | Test Method | Test Result | Unit |
---|
Moisture Absorption | 24hrs | ASTM D-570 | 0.06 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.