Need Help? Contact Us service@plas.com
Get App

PPO NORYL™  EXNL1116-111 SABIC INNOVATIVE US

68
  • Unit Price:
    $3743 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:High temperature resistan Hydrolysis resistance wear resistant
  • Application Areas:valve Mechanical Engineering Instrument panel componen
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Modeling ShrinkageMD:3.20mm内部方法0.50to0.80%
Moisture AbsorptionSaturation,23°CISO620.25%
Moisture AbsorptionEquilibrium,23°C,50%RHISO620.050%
Melt Mass-Flow Rate280°C/5.0kgASTMD12389.6g/10min
Melt Volume flow Rate280°C/5.0kgISO11339.85cm3/10min
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Tensile ElongationYieldASTMD6385.2%
Tensile ModulusASTMD6382170Mpa
Tensile StrengthBreakASTMD63851.3Mpa
Tensile StrengthYieldASTMD63863.3Mpa
Flexural Modulus50.0mmSpanASTMD7902630Mpa
Flexural StrengthYield,50.0mmSpanASTMD790104Mpa
Tensile StressYieldISO527-2/5064.9Mpa
Tensile StressBreakISO527-2/5053.3Mpa
Tensile StrainYieldISO527-2/504.9%
Tensile StrainBreakISO527-2/5021%
Tensile ModulusISO527-2/12910Mpa
Flexural StrengthISO178107Mpa
Tensile ElongationBreakASTMD63829%
Flexural ModulusISO1782630Mpa
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Heat Deflection Temperature1.8MPa,Unannealed,64.0mmSpanISO75-2/Af116°C
Deflection Temperature Under Load?1.8MPa,Unannealed,3.20mmASTMD648115°C
Vicat Softening TemperatureASTMD152510136°C
Vicat Softening Temperature--ISO306/B50136°C
Vicat Softening Temperature--ISO306/B120138°C
Linear thermal expansion coefficientMD:-40to40°CASTME8317.4E-05cm/cm/°C
Linear thermal expansion coefficientMD:-40to40°CISO11359-27.1E-05cm/cm/°C
Linear thermal expansion coefficientTD:-40to40°CASTME8317.1E-05cm/cm/°C
Linear thermal expansion coefficientTD:-40to40°CISO11359-27.4E-05cm/cm/°C
Impact PropertiesTest ConditionTest MethodTest ResultUnit
Instrumented Dart Impact23°C,TotalEnergyASTMD376334.2J
Charpy Notched Impact Strength23°CISO179/1eA16kJ/m²
Notched Izod Impact Strength-30°CISO180/1A7.8kJ/m²
Notched Izod Impact Strength23°CISO180/1A16kJ/m²
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.