Need Help? Contact Us service@plas.com
Get App

PPO NORYL™  EN185-701 SABIC INNOVATIVE US

31
  • Unit Price:
    $3796 USD/MT
  • Packaging Specification:
    25KG/PKG
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Moisture Absorption24 hrASTM D5700.070%
Density / Specific GravityASTM D7921.08g/cm³
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Tensile StrengthYieldASTM D63842.0Mpa
Tensile ElongationBreakASTM D63850%
Flexural Modulus100 mm SpanASTM D7902270Mpa
Flexural StrengthYield, 100 mm SpanASTM D79067.0Mpa
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
RTIUL 74650.0°C
RTI ImpUL 74650.0°C
RTI ElecUL 74650.0°C
Deflection Temperature Under Load?0.45 MPa, Unannealed, 6.40 mmASTM D64893.0°C
Deflection Temperature Under Load?1.8 MPa, Unannealed, 6.40 mmASTM D64882.0°C
Coefficient of Linear Thermal Expansion (Flow)-40 to 95°CASTM E8317.4E-5cm/cm/°C
Electrical performanceTest ConditionTest MethodTest ResultUnit
Comparative Tracking IndexUL 746PLC 2
Hot-wire IgnitionUL 746PLC 1
High Amp Arc IgnitionUL 746PLC 0
High Voltage Arc Tracking RateUL 746PLC 4
Arc ResistanceASTM D495PLC 7
Dielectric Constant60 HzASTM D1502.80
Dielectric Constant50 kHzASTM D1502.80
Dissipation Factor?50 HzASTM D1504.0E-3
Dissipation Factor?60 HzASTM D1504.0E-3
Dissipation Factor?1 MHzIEC 602503.5E-3
Dielectric Strength3.20 mm, in OilASTM D14925KV/mm
ExtrusionTest ConditionTest MethodTest ResultUnit
Drying Temperature90 到 100°C
Drying Time2.0 到 4.0hr
Suggested Max Moisture0.020%
Cylinder Zone 1 Temp170°C
Cylinder Zone 2 Temp170°C
Die Temperature205°C
Cylinder Zone 3 Temp190°C
Cylinder Zone 4 Temp190°C
Adapter Temperature205°C
Melt Temperature195 到 210°C
Impact PropertiesTest ConditionTest MethodTest ResultUnit
Gardner Impact-40°CASTM D302913.0J
Gardner Impact-30°CASTM D302924.0J
Notched Izod Impact Strength-40°CASTM D256160J/m
Notched Izod Impact Strength23°CASTM D256390J/m
hardnessTest ConditionTest MethodTest ResultUnit
Rockwell HardnessR-ScaleASTM D785113
FlammabilityTest ConditionTest MethodTest ResultUnit
Flame Rating1.5 mmUL 94V-1
Flame Rating3.0 mmUL 94V-0
Radiant Panel ListingUL UnspecifiedTRUE
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.