PPO NORYL™  PX9406X-80028 SABIC INNOVATIVE US

73
  • Unit Price:
    $4174 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Flame retardant
  • Application Areas:Electronic communication household electrical appl building materials Automotive interior parts Profile
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Modeling ShrinkageFlow : 3.20 mm内部方法0.50 到 0.70%
Modeling ShrinkageAcross Flow 2内部方法0.50 到 0.70%
Moisture Absorption24 hrASTM D5700.060%
Outdoor SuitabilityUL 746Cf2
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Tensile StrengthYieldASTM D63875.0Mpa
Tensile StrengthBreakASTM D63855.0Mpa
Tensile ElongationYieldASTM D6389.5%
Tensile ElongationBreakASTM D63818%
Flexural Modulus100 mm SpanASTM D7902640Mpa
Flexural StrengthYield, 100 mm SpanASTM D790111Mpa
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Deflection Temperature Under Load?0.45 MPa, Unannealed, 6.40 mmASTM D648133°C
Deflection Temperature Under Load?1.8 MPa, Unannealed, 6.40 mmASTM D648122°C
Vicat Softening TemperatureASTM D15255150°C
RTI ElecUL 746110°C
RTI ImpUL 746105°C
RTIUL 746110°C
Electrical performanceTest ConditionTest MethodTest ResultUnit
Surface ResistivityASTM D257> 1.0E+16ohms
Volume ResistivityASTM D2572.0E+16ohms·cm
Dielectric Strength3.20 mm, in OilASTM D14919KV/mm
Dielectric Constant60 HzASTM D1502.57
Dielectric Constant50 kHzASTM D1502.57
Dielectric Constant1 MHzASTM D1502.49
Dissipation Factor?50 HzASTM D1505.2E-3
Dissipation Factor?60 HzASTM D1505.2E-3
Dissipation Factor?1 MHzASTM D1502.6E-3
Arc ResistanceASTM D495PLC 6
Comparative Tracking IndexUL 746PLC 2
High Amp Arc IgnitionUL 746PLC 0
High Voltage Arc Tracking RateUL 746PLC 4
Hot-wire IgnitionUL 746PLC 0
InjectionTest ConditionTest MethodTest ResultUnit
Drying Temperature105 到 110°C
Drying Time3.0 到 4.0hr
Suggested Max Moisture0.020%
Suggested Shot Size30 到 70%
Rear Temperature245 到 295°C
Middle Temperature255 到 300°C
Front Temperature265 到 305°C
Nozzle Temperature275 到 305°C
Processing (Melt) Temp275 到 305°C
Mold Temperature70 到 100°C
Back Pressure0.300 到 0.700Mpa
Screw Speed20 到 100rpm
Vent Depth0.038 到 0.051mm
Impact PropertiesTest ConditionTest MethodTest ResultUnit
Unnotched Izod Impact Strength23°CASTM D48121100J/m
Instrumented Dart Impact23°C, Energy at PeakASTM D376342.0J
FlammabilityTest ConditionTest MethodTest ResultUnit
Flame Rating0.76 mmUL 94V-0
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.