Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Density | | ASTM D792/ISO 1183 | 1.08 | |
Moisture Absorption 23℃/24H | | ASTM D570/ISO 62 | 0.1 | % |
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Moisture Absorption | 23°C,24hr | ISO62 | 0.10 | % |
Modeling Shrinkage | 2.00mm | 内部方法 | 0.50to0.70 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Flexural Stress | 23°C | ISO178 | 66.0 | Mpa |
Flame Rating | | UL 94 | V-0 | |
Tensile Elongation | | ASTM D-638 | 40 | % |
Nominal Tensile Strain at Break | 23°C | ISO527-2 | 30 | % |
Tensile Stress | | ASTM D-638 | 39 | Mpa |
Tensile Stress | Yield,23°C | ISO527-2 | 37.0 | Mpa |
Tensile Elongation?(Break) | | ASTM D638/ISO 527 | 40 | % |
Tensile Strength | | ASTM D638/ISO 527 | 36 | kg/cm²(MPa)[Lb/in²] |
Rockwell Hardness | | ASTM D785 | R110 | |
Flexural Modulus | | ASTM D790/ISO 178 | 2250 | kg/cm²(MPa)[Lb/in²] |
Flexural Modulus | 23°C | ISO178 | 2370 | Mpa |
Flexural Modulus | | ASTM D-790 | 2350 | Mpa |
Flexural Strength | | ASTM D-790 | 59 | Mpa |
Flexural Strength | | ASTM D790/ISO 178 | 59 | kg/cm²(MPa)[Lb/in²] |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Burning Rate | | UL94 | V-0 | |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ASTMD648 | 85.0 | °C |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ISO75-2/A | 78.0 | °C |
Deflection Temperature Under Load? | | ASTM D648/ISO 75 | 85 | ℃(℉) |
Linear thermal expansion coefficient | MD:-30to65°C | ISO11359-2 | 8E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dielectric Strength | 2.00mm | IEC60243-1 | 29 | KV/mm |
Dissipation Factor? | 1MHz | IEC60250 | 4E-03 | |
Dissipation Factor? | 100Hz | IEC60250 | 3E-03 | |
Surface Resistivity | | IEC60093 | 1E+16 | ohms |
Dielectric Constant | 1MHz | IEC60250 | 2.90 | |
Dielectric Constant | 100Hz | IEC60250 | 2.90 | |
Volume Resistivity | 23°C | IEC60093 | 1E+16 | ohms·cm |
Processing | Test Condition | Test Method | Test Result | Unit |
---|
Mold Temperature | | | 40-70 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Notched Impact Strength | 23°C | ISO179 | 16 | kJ/m² |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 1.5mm | UL94 | V-0 | |
UL flame retardant rating | 3.0mm | UL94 | 5VA | |
Physical | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | | ASTM D-955 | 0.50-0.70 | % |
Moisture Absorption | | ASTM D-570 | 0.10 | % |
Density | | ASTM D-792 | 1.08 | g/cm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.