ECTFE HALAR® 901 SOLVAY USA
122
- Unit Price:
- $14987 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 17MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD | ASTMD955 | 2.5 | % |
Moisture Absorption | Equilibrium | ASTMD570 | <0.10 | % |
Melt Mass-Flow Rate | 275°C/2.16kg | ASTMD1238 | 0.90到1.3 | g/10min |
Density / Specific Gravity | ASTMD792 | 1.68 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Modulus | 23°C | ASTMD790 | 1690 | Mpa |
Tensile Modulus | 23°C | ASTMD638 | 1660 | Mpa |
Coefficient of Friction | Itself - Dynamic | ASTMD1894 | 0.20 | |
Itself - Static | ASTMD1894 | 0.20 | ||
泰伯耐磨性(1000Cycles,500g,CS-17Wheel) | ASTMD1894 | 5.00 | mg | |
Tensile Strength | Yield,23°C | ASTMD638 | 30.0 | Mpa |
Break,23°C | ASTMD638 | 54.0 | Mpa | |
Tensile Elongation | Yield,23°C | ASTMD638 | 5.0 | % |
Break,23°C | ASTMD638 | 250 | % | |
Flexural Strength | 23°C | ASTMD790 | 47.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Linear thermal expansion coefficient | MD | ASTMD696 | 1E-04 | cm/cm/°C |
Melting temperature | ASTMD3418 | 242 | °C | |
Brittleness Temperature | ASTMD746A | <-76.0 | °C | |
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ASTMD648 | 90.0 | °C |
1.8MPa,Unannealed | ASTMD648 | 65.0 | °C | |
Specific Heat | 23°C | ASTMD3418 | 962 | J/kg/°C |
Thermal Conductivity | 40°C | ASTMC177 | 0.15 | W/m/K |
Glass Transition Temperature | DMA | 85.0 | °C | |
Peak Crystallization Temperature? | DSC | ASTMD3418 | 222 | °C |
Peak Crystallization Temperature? | ASTMD3418 | 42.0 | J/g | |
Peak Crystallization Temperature | ASTMD3418 | 40.0 | J/g | |
热稳定性-1%质量损失,N2 | TGA | 405 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Volume Resistivity | 23°C | ASTMD257 | 5.5E+16 | ohms·cm |
Dielectric Constant | 23°C,1MHz | ASTMD150 | 2.57 | |
Dielectric Strength | 23°C,3.20mm | ASTMD149 | 14 | KV/mm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Notched Izod Impact Strength | -40°C,3.20mm | ASTMD256 | 210 | J/m |
23°C,3.20mm | ASTMD256 | 无断裂 |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | R-Scale | ASTMD785 | 90 | |
Shore Hardness | Shore D | ASTMD2240 | 75 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | UL94 | V-0 | ||
Oxygen Index | ASTMD2863 | 52 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.