PAI TORLON® 4301 SOLVAY USA
111
- Unit Price:
- $166061 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:--
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD | ASTMD955 | 0.35到0.60 | % |
Water absorption rate | 24hr | ASTMD570 | 0.28 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | -- | ASTMD638 | 6830 | Mpa |
--2 | ASTMD1708 | 6550 | Mpa | |
Tensile strength | ASTMD638 | 113 | Mpa | |
Tensile stress 3 | ASTMD1708 | 163 | Mpa | |
elongation | Break | ASTMD638 | 3.3 | % |
Break2 | ASTMD1708 | 7.0 | % | |
Bending modulus | 23°C | ASTMD790 | 6890 | Mpa |
232°C | ASTMD790 | 4960 | Mpa | |
bending strength | 23°C | ASTMD790 | 215 | Mpa |
232°C | ASTMD790 | 112 | Mpa | |
Compressive modulus | ASTMD695 | 5310 | Mpa | |
compressive strength | ASTMD695 | 166 | Mpa | |
friction coefficient | --4 | ASTMD3702 | 0.31 | |
--5 | ASTMD3702 | 0.39 | ||
--6 | ASTMD3702 | 0.18 | ||
--7 | ASTMD3702 | 0.030 | ||
Wear factor | 干燥:4m/s,0.2MPa(800fpm,31.25psi) | ASTMD3702 | 17.0 | in³·min^-10/ft·lb·hr |
干燥:0.25m/s,3.4MPa(50fpm,500psi) | ASTMD3702 | 14.0 | in³·min^-10/ft·lb·hr | |
润滑:0.25m/s,6.9MPa(75fpm,1000psi) | ASTMD3702 | 9.00 | in³·min^-10/ft·lb·hr | |
润滑:4m/s,5.2MPa(800fpm,750psi) | ASTMD3702 | 0.400 | in³·min^-10/ft·lb·hr |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ASTMD648 | 279 | °C |
thermal conductivity | ASTMC177 | 0.53 | W/m/K | |
Linear coefficient of thermal expansion | ASTMD696 | 2.5E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistivity | ASTMD257 | 8E+17 | ohms | |
Volume resistivity | ASTMD257 | 8E+15 | ohms·cm |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Cantilever beam without notch impact strength | ASTMD256 | 410 | J/m |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.