Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Moisture Absorption | 24 hr, 23°C | ISO 62 | 0.30 | % |
Modeling Shrinkage (Flow) | | 内部方法 | 0.10 到 0.40 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Stress | Break | ISO 527-2 | 230 | Mpa |
Tensile Strain | Break | ISO 527-2 | 2.5 | % |
Tensile Modulus | | ISO 527-2 | 13000 | Mpa |
Flexural Modulus | | ISO 178 | 11000 | Mpa |
Flexural Stress | | ISO 178 | 320 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 1.8 MPa, Unannealed | ISO 75-2/A | 230 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dielectric Constant | 2.40 GHz | ASTM D2520 | 3.50 | |
Dissipation Factor? | 2.40 GHz | ASTM D2520 | 0.010 | |
Injection | Test Condition | Test Method | Test Result | Unit |
---|
Drying Temperature | | | 120 | °C |
Processing (Melt) Temp | | | 280 到 300 | °C |
Mold Temperature | | | 120 到 140 | °C |
Drying Time | | | 0.50 到 1.5 | hr |
Rear Temperature | | | 250 到 260 | °C |
Front Temperature | | | 260 到 290 | °C |
Injection Rate | | | 快速 | |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Notched Izod impact strength | | ISO 180 | 40 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.