ASA/PC GELOY™  XP4034 SABIC INNOVATIVE US

179
  • Unit Price:
    $2821 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    20MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:High mobility Thermal stability Antistatic Weather resistance
  • Application Areas:Automotive sector
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Modeling ShrinkageFlow : 3.20 mm内部方法0.50 到 0.70%
Modeling ShrinkageAcross Flow : 3.20 mm内部方法0.50 到 0.70%
Moisture Absorption24 hrASTM D5700.25%
Melt Mass-Flow Rate220°C/10.0 kgASTM D12385.0g/10 min
Melt Mass-Flow Rate260°C/5.0 kgASTM D123814g/10 min
Melt Mass-Flow Rate280°C/3.8 kgASTM D123824g/10 min
Outdoor SuitabilityUL 746Cf2
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Tensile StrainYieldISO 527-2/504.5%
Tensile StrainBreak 2ASTM D63825%
Tensile StrainBreakISO 527-2/50130%
Tensile ModulusISO 527-2/12500Mpa
Flexural Modulus50.0 mm Span 3ASTM D7902510Mpa
Flexural Modulus-- 4ISO 1782500Mpa
Tensile StrengthYield 2ASTM D63862.0Mpa
Tensile StrengthYieldISO 527-2/5057.0Mpa
Tensile StrengthBreakISO 527-2/5050.0Mpa
Flexural Stress-- 4, 5ISO 17875.0Mpa
Flexural StressYield, 50.0 mm Span 3ASTM D79088.0Mpa
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Thermal ConductivityASTM C1770.25W/m/K
Vicat Softening TemperatureISO 306/B50113°C
Linear thermal expansion coefficientFlow : -20 to 150°CASTM E8317.2E-5cm/cm/°C
Linear thermal expansion coefficientAcross Flow : -20 to 150°CASTM E8317.2E-5cm/cm/°C
Deflection Temperature Under Load?0.45 MPa, Unannealed, 3.20 mmASTM D648115°C
Deflection Temperature Under Load?0.45 MPa, Unannealed, 4.00 mm, 64.0 mm Span 7ISO 75-2/Bf116°C
Deflection Temperature Under Load?1.8 MPa, Unannealed, 6.40 mmASTM D648104°C
Deflection Temperature Under Load?1.8 MPa, Unannealed, 4.00 mm, 64.0 mm Span 7ISO 75-2/Af98.0°C
InjectionTest ConditionTest MethodTest ResultUnit
Drying Time3.0 到 4.0hr
Suggested Shot Size40 到 80%
Rear Temperature240 到 255°C
Middle Temperature245 到 260°C
Front Temperature250 到 265°C
Nozzle Temperature245 到 265°C
Back Pressure0.300 到 1.00Mpa
Screw Speed30 到 80rpm
Vent Depth0.038 到 0.076mm
Drying Temperature95 到 105°C
Suggested Max Moisture0.040%
Processing (Melt) Temp260 到 275°C
Mold Temperature55 到 70°C
Impact PropertiesTest ConditionTest MethodTest ResultUnit
Instrumented Dart Impact-30°C, Total EnergyASTM D376330.0J
Instrumented Dart Impact23°C, Total EnergyASTM D376347.0J
hardnessTest ConditionTest MethodTest ResultUnit
Rockwell HardnessR-ScaleASTM D785110
optical performance Test ConditionTest MethodTest ResultUnit
Gardner60°, 无织构ASTM D52394
FlammabilityTest ConditionTest MethodTest ResultUnit
Flame Rating1.5 mmUL 94HB
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.