Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD:3.00mm | ASTMD955 | 0.80 | % |
Moisture Absorption | 24hr,3.18mm | ASTMD570 | 0.26 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Elongation | Break | ASTMD638 | 60 | % |
Flexural Modulus | | ASTMD790 | 2100 | Mpa |
Flexural Strength | | ASTMD790 | 84.0 | Mpa |
Compressive Strength | | ASTMD695 | 84.0 | Mpa |
Tensile Strength | | ASTMD638 | 69.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ASTMD648 | 175 | °C |
Linear thermal expansion coefficient | MD | ASTMD696 | 6.1E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dielectric Strength | | ASTMD149 | 39 | KV/mm |
Comparative Tracking Index | | IEC60112 | 220 | V |
Dielectric Constant | 1MHz | ASTMD150 | 3.00 | |
Arc Resistance | | ASTMD495 | 130 | sec |
Volume Resistivity | | ASTMD257 | 2E+16 | ohms·cm |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | R-Scale | ASTMD785 | 125 | |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Transmittance | 3000µm | ASTMD1003 | 87.0 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.