PC/PBT XENOY™ 357-GY8D697 SABIC INNOVATIVE SHANGHAI
94
- Unit Price:
- $3874 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 33MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Impact modification
- Application Areas:Electronic display Industrial applications switch Shell Spool medical care Lighting fixtures
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | TD:--3 | 内部方法 | 1.2to1.6 | % |
MD:--2 | 内部方法 | 0.80to1.1 | % | |
MD:--3 | 内部方法 | 1.0to1.4 | % | |
MD:3.20mm | 内部方法 | 1.0to1.4 | % | |
TD:--2 | 内部方法 | 0.90to1.3 | % | |
Moisture Absorption | 24hr | ASTMD570 | 0.080 | % |
Saturation,23°C | ISO62 | 0.50 | % | |
Equilibrium,23°C,50%RH | ISO62 | 0.15 | % | |
Melt Mass-Flow Rate | 250°C/5.0kg | ASTMD1238 | 9.6 | g/10min |
Melt Volume flow Rate | 250°C/5.0kg | ISO1133 | 8.00 | cm3/10min |
Specific Volume | ASTMD792 | 0.740 | cm³/g | |
Outdoor Suitability | UL746C | f2 | ||
Density / Specific Gravity | ASTMD792 | 1.35 | g/cm³ | |
ISO1183 | 1.34 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Strain | Break | ASTMD638 | 54 | % |
Yield | ASTMD638 | 5.0 | % | |
Flexural Modulus | 50.0mmSpan | ASTMD790 | 2100 | Mpa |
ISO178 | 2000 | Mpa | ||
Flexural Strength | ISO178 | 73.0 | Mpa | |
Flexural Strength | Yield,50.0mmSpan | ASTMD790 | 78.0 | Mpa |
Flexural Strength | Break,50.0mmSpan | ASTMD790 | 78.0 | Mpa |
Tensile Stress | Yield | ISO527-2/50 | 50.0 | Mpa |
Break | ISO527-2/50 | 40.0 | Mpa | |
Tensile Strain | Yield | ISO527-2/50 | 5.0 | % |
Break | ISO527-2/50 | 30 | % | |
Tensile Modulus | ISO527-2/1 | 2200 | Mpa | |
Tensile Modulus | ASTMD638 | 2020 | Mpa | |
Tensile Strength | Yield | ASTMD638 | 48.0 | Mpa |
Tensile Strength | Break | ASTMD638 | 42.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed,3.20mm | ASTMD648 | 135 | °C |
0.45MPa,Unannealed,6.40mm | ASTMD648 | 138 | °C | |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 98.0 | °C | |
1.8MPa,Unannealed,6.40mm | ASTMD648 | 99.0 | °C | |
Linear thermal expansion coefficient | MD:-40to40°C | ASTME831 | 9.2E-05 | cm/cm/°C |
MD:60to138°C | ASTME831 | 1.2E-04 | cm/cm/°C | |
MD:-40to40°C | ISO11359-2 | 7.2E-05 | cm/cm/°C | |
TD:-40to40°C | ASTME831 | 8.4E-05 | cm/cm/°C | |
TD:-40to40°C | ISO11359-2 | 8.4E-05 | cm/cm/°C | |
RTIElec | UL746 | 120 | °C | |
Evolution Calendar intelligent importer | UL746 | 120 | °C | |
RTIStr | UL746 | 140 | °C | |
Heat Deflection Temperature | 1.8MPa,Unannealed,64.0mmSpan | ISO75-2/Af | 84.0 | °C |
Ball PressureTest | 125°C | IEC60695-10-2 | Pass | |
Vicat Softening Temperature | ASTMD152513 | 134 | °C | |
-- | ISO306/B50 | 145 | °C | |
-- | ISO306/B120 | 150 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot-wire Ignition | HWI | UL746 | PLC2 | |
High Amp Arc Ignition | HAI | UL746 | PLC3 | |
High Voltage Arc Tracking Rate | HVTR | UL746 | PLC3 | |
Comparative Tracking Index | CTI | UL746 | PLC2 | |
Dissipation Factor? | 100Hz | ASTMD150 | 3E-03 | |
1MHz | ASTMD150 | 0.030 | ||
Dielectric Strength | 1.60mm,in Oil | ASTMD149 | 25 | KV/mm |
3.20mm,inAir | ASTMD149 | 19 | KV/mm | |
3.20mm,in Oil | ASTMD149 | 19 | KV/mm | |
Dielectric Constant | 100Hz | ASTMD150 | 3.20 | |
1MHz | ASTMD150 | 3.20 | ||
Volume Resistivity | ASTMD257 | >1.2E+16 | ohms·cm | |
Arc Resistance | ASTMD495 | PLC6 |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Gardner Impact | 23°C | ASTMD3029 | 43.4 | J |
23°C11 | ASTMD3029 | 43.0 | J | |
Instrumented Dart Impact | 23°C,TotalEnergy | ASTMD3763 | 35.8 | J |
Notched Izod Impact Strength | 23°C | ASTMD4812 | NoBreak | |
-30°C | ASTMD256 | 150 | J/m | |
23°C | ASTMD256 | 320 | J/m | |
CharpyNotchedImpactStrength9 | 23°C | ISO179/1eA | 45 | kJ/m² |
Notched Izod Impact Strength | -30°C | ISO180/1A | 10 | kJ/m² |
23°C | ISO180/1A | 45 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | R-Scale | ASTMD785 | 117 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.46mm | UL94 | HB | |
0.63mm | UL94 | V-0 | ||
3.0mm | UL94 | 5VA | ||
Glow Wire Flammability Index | 1.0mm | IEC60695-2-12 | 960 | °C |
Glow Wire Ignition Temperature | 1.0mm | IEC60695-2-13 | 775 | °C |
2.0mm | IEC60695-2-13 | 750 | °C | |
3.0mm | IEC60695-2-13 | 725 | °C | |
Oxygen Index | ASTMD2863 | 30 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.