PC/PBT VALOX™ 553U-1001 SABIC INNOVATIVE SHANGHAI
95
- Unit Price:
- $3684 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 31MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Chemical resistance Low temperature impact re Filler: Glass fiber reinf 30% Filler by weight
- Application Areas:Handle Pump parts Motor casing Electronic display Home appliance components Household daily necessiti Shell Lighting applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:--2 | 内部方法 | 0.30to0.50 | % |
MD:--3 | 内部方法 | 0.50to0.80 | % | |
TD:--2 | 内部方法 | 0.40to0.60 | % | |
TD:--4 | 内部方法 | 0.60to0.90 | % | |
Moisture Absorption | 24hr | ASTMD570 | 0.070 | % |
Specific Volume | ASTMD792 | 0.636 | cm³/g | |
Outdoor Suitability | UL746C | f1 |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Modulus | 50.0mmSpan | ASTMD790 | 6890 | Mpa |
Flexural Strength | Break,50.0mmSpan | ASTMD790 | 179 | Mpa |
Tensile Strength | Break | ASTMD638 | 110 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed,6.40mm | ASTMD648 | 204 | °C |
1.8MPa,Unannealed,6.40mm | ASTMD648 | 160 | °C | |
RTIElec | UL746 | 125 | °C | |
Evolution Calendar intelligent importer | UL746 | 110 | °C | |
RTIStr | UL746 | 125 | °C | |
Linear thermal expansion coefficient | MD:-40to40°C | ASTME831 | 2.2E-05 | cm/cm/°C |
MD:60to138°C | ASTME831 | 2.2E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric Strength | 1.60mm,in Oil | ASTMD149 | 26 | KV/mm |
3.20mm,inAir | ASTMD149 | 19 | KV/mm | |
Comparative Tracking Index | CTI | UL746 | PLC3 | |
Arc Resistance | ASTMD495 | PLC6 | ||
Dissipation Factor? | 100Hz | ASTMD150 | 2E-03 | |
1MHz | ASTMD150 | 0.020 | ||
Dielectric Constant | 100Hz | ASTMD150 | 3.80 | |
1MHz | ASTMD150 | 3.70 | ||
Volume Resistivity | ASTMD257 | 4.3E+16 | ohms·cm | |
Hot-wire Ignition | HWI | UL746 | PLC1 | |
High Amp Arc Ignition | HAI | UL746 | PLC3 | |
High Voltage Arc Tracking Rate | HVTR | UL746 | PLC3 |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | R-Scale | ASTMD785 | 118 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Oxygen Index | ASTMD2863 | 37 | % | |
UL flame retardant rating | 0.9mm | UL94 | V-0 | |
2.3mm | UL94 | 5VA |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.