TPEE Hytrel® HTR8223 BK320 DUPONT USA
84
- Unit Price:
- $3128 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 50MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High temperature resistan Chemical resistance
- Application Areas:Blow molding applications Cable Automotive Applications
- Color:--
- Grade:Withdrawal level
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Moisture Absorption | 23°C,24hr | ISO62 | 0.60 | % |
Saturation,23°C,2.00mm | ISO62 | 0.80 | % | |
Equilibrium,23°C,2.00mm,50%RH | ISO62 | 0.20 | % | |
Modeling Shrinkage | TD | ISO294-4 | 1.6 | % |
MD | ISO294-4 | 1.6 | % | |
Melt Mass-Flow Rate | 230°C/10.0kg | ISO1133 | 9.5 | g/10min |
MediumDensity | 0.980 | g/cm³ | ||
Melt Volume flow Rate | 230°C/10.0kg | ISO1133 | 10.0 | cm3/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Nominal Tensile Strain at Break | ISO527-2 | 680 | % | |
Abrasion Resistance | ISO4649 | 22.0 | mm³ | |
Tensile Modulus | ISO527-2 | 75.0 | Mpa | |
Flexural Modulus | ISO178 | 79.0 | Mpa | |
Tensile Stress | Break | ISO527-2 | 26.0 | Mpa |
5.0%Strain | ISO527-2 | 3.50 | Mpa | |
10%Strain | ISO527-2 | 5.50 | Mpa | |
50%Strain | ISO527-2 | 10.0 | Mpa | |
100%Strain | ISO527-2 | 13.0 | Mpa | |
300%Strain | ISO527-2 | 19.0 | Mpa | |
Tensile Strain | Break | ISO527-2 | >300 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Brittleness Temperature | ISO974 | -100 | °C | |
Linear thermal expansion coefficient | MD | ISO11359-2 | 1.7E-04 | cm/cm/°C |
TD | ISO11359-2 | 1.7E-04 | cm/cm/°C | |
Melting Temperature | ISO11357-3 | 195 | °C | |
Glass Transition Temperature | ISO11357-2 | -50.0 | °C | |
Effective Thermal Diffusivity | 5.44E-08 | m²/s |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Comparative Tracking Index | IEC60112 | 600 | V | |
Dielectric Strength | IEC60243-1 | 18 | KV/mm | |
Surface Resistivity | IEC60093 | 2E+14 | ohms | |
Volume Resistivity | IEC60093 | 9E+12 | ohms·cm | |
Dissipation Factor? | 100Hz | IEC60250 | 7E-03 | |
1MHz | IEC60250 | 0.013 |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore Hardness | Shore D | ISO868 | 42 | |
Shore D,15sec | ISO868 | 38 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
FMVSS Flammability | FMVSS302 | B | ||
Burning Rate | 1.00mm | ISO3795 | <100 | mm/min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.