Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD:3.20mm | ASTMD955 | 1.3to1.7 | % |
Moisture Absorption | 23°C,24hr | ASTMD570 | 0.30 | % |
Melt Mass-Flow Rate | 230°C/2.16kg | ASTMD1238 | 24 | g/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Flexural Modulus | 6.40mm | ASTMD790 | 324 | Mpa |
Tensile Elongation | Break,2.00mm | ASTMD638 | 650 | % |
Tensile Strength | Yield,2.00mm | ASTMD638 | 18.6 | Mpa |
Tensile Strength | Break,2.00mm | ASTMD638 | 49.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed,6.40mm | ASTMD648 | 111 | °C |
Peak Melting Temperature | | ASTMD3418 | <212 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Comparative Tracking Index | SolutionA | IEC60112 | 600 | V |
Volume Resistivity | | ASTMD257 | >1.0E+13 | ohms·cm |
Dielectric Strength | 23°C,1.00mm | ASTMD149 | 26 | KV/mm |
Elastomers Properties | Test Condition | Test Method | Test Result | Unit |
---|
TearStrength2,4 | | ASTMD624 | 157 | kN/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Shore Hardness | Shore D | ASTMD2240 | 61 | |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 1.5mm | UL94 | HB | |
UL flame retardant rating | 3.0mm | UL94 | HB | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.