Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD:3.20mm,InjectionMolded | ASTMD955 | 0.60to1.0 | % |
Moisture Absorption | 23°C,24hr | ASTMD570 | 0.60 | % |
Melt Mass-Flow Rate | 230°C/2.16kg | ASTMD1238 | 25 | g/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Flexural Modulus | 6.40mm | ASTMD790 | 78.5 | Mpa |
Tensile Elongation | Break,2.00mm | ASTMD638 | 800 | % |
Tensile Strength | Break,2.00mm | ASTMD638 | 29.4 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Peak Melting Temperature | | ASTMD3418 | 180 | °C |
Deflection Temperature Under Load? | 0.45MPa,Unannealed,6.40mm,Injection | ASTMD648 | 65.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Volume Resistivity | 23°C | ASTMD257 | >1.0E+13 | ohms·cm |
Dielectric Strength | 23°C,1.00mm | ASTMD149 | 26 | KV/mm |
Comparative Tracking Index | SolutionA | IEC60112 | 600 | V |
Elastomers Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tearing Strength | 23°C | ASTMD624 | 104 | kN/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Shore Hardness | Shore A,23°C,Injection | ASTMD2240 | 95 | |
Shore Hardness | Shore D,23°C,Injection | ASTMD2240 | 42 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.