Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD | ASTMD955 | 0.40 | % |
Modeling Shrinkage | TD | ASTMD955 | 0.80 | % |
Moisture Absorption | 24hr | ASTMD570 | 0.21 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Stress | Yield | ISO527-2 | 225 | Mpa |
Tensile Strain | Break | ISO527-2 | 3.0 | % |
Tensile Modulus | | ASTMD638 | 13100 | Mpa |
Tensile Modulus | | ISO527-2 | 12200 | Mpa |
Tensile Elongation | Break | ASTMD638 | 2.5 | % |
Flexural Modulus | | ASTMD790 | 10300 | Mpa |
Flexural Modulus | | ISO178 | 10300 | Mpa |
Flexural Strength | Yield | ASTMD790 | 317 | Mpa |
Flexural Stress | | ISO178 | 326 | Mpa |
Compressive Strength | | ASTMD695 | 276 | Mpa |
Shearing Strength | | ASTMD732 | 101 | Mpa |
Poisson Ratio | | 7.58 | 0.41 | |
Tensile Strength | Break | ASTMD638 | 221 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Peak Melting Temperature | | ASTMD3418 | 310 | °C |
Continuous Use Temperature | --2 | ASTMD3045 | 164 | °C |
Continuous Use Temperature | --3 | ASTMD3045 | 185 | °C |
Deflection Temperature Under Load? | 0.45MPa,Annealed,3.18mm | ASTMD648 | 297 | °C |
Deflection Temperature Under Load? | 1.8MPa,Annealed,3.18mm | ASTMD648 | 285 | °C |
Deflection Temperature Under Load? | 1.8MPa,Annealed | ISO75-2/Af | 277 | °C |
Linear thermal expansion coefficient | MD:0to100°C | ASTME831 | 2.3E-05 | cm/cm/°C |
Linear thermal expansion coefficient | MD:160to249°C | ASTME831 | 1.4E-05 | cm/cm/°C |
Linear thermal expansion coefficient | TD:0to100°C | ASTME831 | 5.9E-05 | cm/cm/°C |
Linear thermal expansion coefficient | TD:160to249°C | ASTME831 | 1.3E-04 | cm/cm/°C |
Melting temperature | | ISO11357-3 | 310 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dielectric Constant | 60Hz | ASTMD150 | 4.40 | |
Dielectric Constant | 1MHz | ASTMD150 | 4.20 | |
Arc Resistance | | ASTMD495 | 140 | sec |
Volume Resistivity | | ASTMD257 | 1E+16 | ohms·cm |
Dielectric Strength | 3.17mm | ASTMD149 | 21 | KV/mm |
Dissipation Factor? | 60Hz | ASTMD150 | 5E-03 | |
Dissipation Factor? | 1MHz | ASTMD150 | 0.017 | |
Comparative Tracking Index | CTI | UL746 | 550 | V |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Unnotched Impact Strength | | ISO179/1eU | 82 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | R-Scale | ASTMD785 | 125 | |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Light Transmittance | 1070nm:1.60mm | ASTMD1003 | >35 | % |
Light Transmittance | 940nm:1.60mm | ASTMD1003 | >30 | % |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
Flame Rating | 3.2mm | UL94 | HB | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.