TPV Santoprene™ 291-60B150 CELANESE USA
41
- Unit Price:
- $8667 USD/MT
- Packaging Specification:
- 25KG/PKG
- Supply Quantity:
- 30MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Technical Data Sheet
Aging Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Change in Tensile Strength | 23°C,168hr,inHydrochloricAcid,10% | ASTMD471 | -20 | % |
23°C,168hr,inRelativeHumidity,90% | ASTMD471 | -11 | % | |
23°C,168hr,inSodiumChloride,15% | ASTMD471 | -18 | % | |
23°C,168hr,inSodiumHydroxide,50% | ASTMD471 | -22 | % | |
38°C,168hr,inRelativeHumidity,90% | ASTMD471 | -16 | % | |
23°C,24hr,inIRM903Oil | ISO1817 | -4.0 | % | |
23°C,168hr,inCascadeDetergent | ISO1817 | -20 | % | |
23°C,168hr,inClorox,10% | ISO1817 | -16 | % | |
23°C,168hr,inEthanol,50% | ISO1817 | -65 | % | |
23°C,168hr,inHydrochloricAcid,10% | ISO1817 | -20 | % | |
23°C,24hr,inIRM903Oil | ASTMD471 | -4.0 | % | |
23°C,168hr,inCascadeDetergent | ASTMD471 | -20 | % | |
23°C,168hr,inClorox,10% | ASTMD471 | -16 | % | |
23°C,168hr,inEthanol,50% | ASTMD471 | -65 | % | |
23°C,168hr,inRelativeHumidity,90% | ISO1817 | -11 | % | |
23°C,168hr,inSodiumChloride,15% | ISO1817 | -18 | % | |
23°C,168hr,inSodiumHydroxide,50% | ISO1817 | -22 | % | |
38°C,168hr,inRelativeHumidity,90% | ISO1817 | -16 | % | |
Change in Mass | 23°C,168hr,inCascadeDetergent | ASTMD471 | 0.10 | % |
23°C,168hr,inClorox,10% | ASTMD471 | 0.60 | % | |
23°C,168hr,inEthanol,50% | ASTMD471 | 6.5 | % | |
23°C,168hr,inHydrochloricAcid,10% | ASTMD471 | 0.40 | % | |
23°C,168hr,inRelativeHumidity,95% | ASTMD471 | 0.0 | % | |
23°C,168hr,inSodiumChloride,15% | ASTMD471 | 0.10 | % | |
23°C,168hr,inSodiumHydroxide,50% | ASTMD471 | 0.10 | % | |
38°C,168hr,inRelativeHumidity,95% | ASTMD471 | 0.60 | % | |
23.0°C,168hr,inRelativeHumidity,95% | ISO1817 | 0.0 | % | |
23.0°C,168hr,inSodiumChloride,15% | ISO1817 | 0.10 | % | |
23.0°C,168hr,inCascadeDetergent | ISO1817 | 0.10 | % | |
23.0°C,168hr,inSodiumHydroxide,50% | ISO1817 | 0.10 | % | |
23.0°C,168hr,inHydrochloricAcid,10% | ISO1817 | 0.40 | % | |
38.0°C,168hr,inRelativeHumidity,95% | ISO1817 | 0.60 | % | |
23.0°C,168hr,inClorox,10% | ISO1817 | 0.60 | % | |
23.0°C,168hr,inEthanol,50% | ISO1817 | 6.5 | % | |
Tensile Stress(Break) | 23°C,24hr,inIRM903Oil | ISO1817 | -4.0-4.0-4.0-4.0-4.0 | % |
23°C,168hr,inCascadeDetergent | ISO1817 | -7.0 | % | |
23°C,168hr,inClorox,10% | ISO1817 | -4.0 | % | |
23°C,168hr,inEthanol,50% | ISO1817 | -66 | % | |
23°C,168hr,inHydrochloricAcid,10% | ISO1817 | -10 | % | |
23°C,168hr,inRelativeHumidity,90% | ISO1817 | -10 | % | |
23°C,168hr,inSodiumChloride,15% | ISO1817 | -6.0 | % | |
23°C,168hr,inSodiumHydroxide,50% | ISO1817 | -18 | % | |
38°C,168hr,inRelativeHumidity,90% | ISO1817 | -9.0 | % | |
Change in Volume | 23°C,168hr,inEthanol,50% | ISO1817 | 6.8 | % |
23°C,168hr,inHydrochloricAcid,10% | ISO1817 | 0.40 | % | |
23°C,168hr,inRelativeHumidity,95% | ISO1817 | 0.0 | % | |
23°C,168hr,inSodiumChloride,15% | ISO1817 | 0.60 | % | |
23°C,168hr,inSodiumHydroxide,50% | ISO1817 | 0.20 | % | |
38°C,168hr,inRelativeHumidity,95% | ISO1817 | 0.60 | % | |
23°C,168hr,inCascadeDetergent | ASTMD471 | 0.10 | % | |
23°C,168hr,inClorox,10% | ASTMD471 | 0.60 | % | |
23°C,168hr,inEthanol,50% | ASTMD471 | 6.8 | % | |
23°C,168hr,inHydrochloricAcid,10% | ASTMD471 | 0.40 | % | |
23°C,168hr,inRelativeHumidity,95% | ASTMD471 | 0.0 | % | |
23°C,168hr,inSodiumChloride,15% | ASTMD471 | 0.60 | % | |
23°C,168hr,inSodiumHydroxide,50% | ASTMD471 | 0.20 | % | |
38°C,168hr,inRelativeHumidity,95% | ASTMD471 | 0.60 | % | |
23°C,168hr,inCascadeDetergent | ISO1817 | 0.10 | % | |
23°C,168hr,inClorox,10% | ISO1817 | 0.60 | % | |
ChangeinShoreHardness | ShoreA,23°C,168hr,inDeionizedWater | ISO1817 | -1.0 | |
Change in Ultimate Elongation | 23°C,24hr,inIRM903Oil | ASTMD471 | -4.0-4.0-4.0-4.0-4.0 | % |
23°C,168hr,inCascadeDetergent | ASTMD471 | -7.0 | % | |
23°C,168hr,inClorox,10% | ASTMD471 | -4.0 | % | |
23°C,168hr,inEthanol,50% | ASTMD471 | -66 | % | |
23°C,168hr,inHydrochloricAcid,10% | ASTMD471 | -10 | % | |
23°C,168hr,inRelativeHumidity,90% | ASTMD471 | -10 | % | |
23°C,168hr,inSodiumChloride,15% | ASTMD471 | -6.0 | % | |
23°C,168hr,inSodiumHydroxide,50% | ASTMD471 | -18 | % | |
38°C,168hr,inRelativeHumidity,90% | ASTMD471 | -9.0 | % | |
Change in Tensile Strength in Air | 100°C,168hr | ASTMD573 | 0.0 | % |
100°C,168hr | ISO188 | 0.0 | % | |
ChangeinUltimateElongationinAir | 100°C,168hr | ASTMD573 | -11 | % |
Change in Durometer Hardness in Air | ShoreA,100°C,672hr | ASTMD573 | -2.0 | |
Change in Shore Hardness in Air | ShoreA,100°C,672hr | ISO188 | -2.0 | |
ChangeinMassinAir | 100°C,168hr | ASTMD573 | -1.1 | % |
100°C,168hr | ISO188 | -1.1 | % | |
ChangeInvoiceinair | 100°C,168hr | ASTMD573 | -1.2 | % |
100°C,168hr | ISO188 | -1.2 | % | |
change | ShoreA,23°C,168hr,inDeionizedWater | ASTMD471 | -1.0 |
Elastomers Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress(Across Flow) | 100%Strain,23°C | ASTMD412 | 2.10 | Mpa |
100%Strain,23°C | ISO37 | 2.10 | Mpa | |
Tensile Strength (flow) | Break,23°C | ASTMD412 | 8.00 | Mpa |
Tensile Strength (TD) | Break,23°C | ISO37 | 8.00 | Mpa |
Tensile Elongation(Across Flow) | Break,23°C | ASTMD412 | 540 | % |
Break,23°C | ISO37 | 540 | % | |
Compression Set | 23°C,22hr | ASTMD395B | 34 | % |
70°C,22hr | ASTMD395B | 62 | % | |
Compression Set | 23°C,22hr | ISO815 | 34 | % |
70°C,22hr | ISO815 | 62 | % | |
Tearing Strength (MD) | 23°C | ASTMD624 | 28.0 | kN/m |
TearStrength-AcrossFlow3 | 23°C | ISO34-1 | 28 | kN/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore Hardness | Shore A,15sec,23°C | ISO868 | 65 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.