Need Help? Contact Us service@plas.com
Get App

TPV Santoprene™ 8211-55B100 CELANESE USA

57
  • Unit Price:
    $6924 USD/MT
  • Packaging Specification:
    25KG/PKG
  • Supply Quantity:
    42MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Technical Data Sheet

Aging PropertiesTest ConditionTest MethodTest ResultUnit
Change in Tensile Strength23°C,168hr,inEthanol,95%ASTMD471-17%
Change in Tensile Strength23°C,168hr,inHydrochloricAcid,10%ASTMD471-1.0%
Change in Tensile Strength23°C,168hr,inIRM903OilASTMD471-85%
Change in Tensile Strength23°C,168hr,inSodiumHydroxide,50%ASTMD4711.0%
Change in Tensile Strength23°C,168hr,在水中ASTMD4712.0%
Change in Tensile Strength23°C,168hr,inEthanol,95%ISO1817-17%
Change in Tensile Strength23°C,168hr,inHydrochloricAcid,10%ISO1817-1.0%
Change in Tensile Strength23°C,168hr,inIRM903OilISO1817-85%
Change in Tensile Strength23°C,168hr,inSodiumHydroxide,50%ISO18171.0%
Change in Tensile Strength23°C,168hr,在水中ISO18172.0%
Change in Tensile Strength in Air100°C,168hrASTMD573-28%
Change in Tensile Strength in Air125°C,168hrASTMD573-61%
Change in Tensile Strength in Air100°C,168hrISO188-28%
Change in Tensile Strength in Air125°C,168hrISO188-61%
Change in Tensile Strain at Break in Air?100°C,168hrISO188-14%
Change in Tensile Strain at Break in Air?125°C,168hrISO188-70%
Tensile Stress(Break)23°C,168hr,inEthanol,95%ISO1817-3.0%
Tensile Stress(Break)23°C,168hr,inHydrochloricAcid,10%ISO1817-9.0%
Tensile Stress(Break)23°C,168hr,inIRM903OilISO1817-68%
Tensile Stress(Break)23°C,168hr,inSodiumHydroxide,50%ISO1817-7.0%
Tensile Stress(Break)23°C,168hr,在水中ISO1817-12%
Change in Durometer Hardness in AirShoreA,100°C,168hrASTMD573-4.0
Change in Durometer Hardness in AirShore A,125°C,168hrASTMD5738.0
Change in Ultimate Elongation in Air100°C,168hrASTMD573-14%
Change in Ultimate Elongation in Air125°C,168hrASTMD573-70%
Change in Shore Hardness in AirShoreA,100°C,168hrISO188-4.0
Change in Shore Hardness in AirShore A,125°C,168hrISO1888.0
Change in Durometer HardnessShoreA,23°C,168hr,inIRM903OilASTMD471-33
Change in Durometer HardnessShoreA,23°C,168hr,inSodiumHydroxide,50%ASTMD4714.0
Change in Durometer HardnessShoreA,23°C,168hr,inWaterASTMD4715.0
Change in Durometer HardnessShoreA,23°C,168hr,inEthanol,95%ASTMD4712.0
Change in Durometer HardnessShoreA,23°C,168hr,inHydrochloricAcid,10%ASTMD4714.0
ChangeinShoreHardnessShoreA,23°C,168hr,inEthanol,95%ISO18172.0
ChangeinShoreHardnessShoreA,23°C,168hr,inHydrochloricAcid,10%ISO18174.0
ChangeinShoreHardnessShoreA,23°C,168hr,inIRM903OilISO1817-33
ChangeinShoreHardnessShoreA,23°C,168hr,inSodiumHydroxide,50%ISO18174.0
ChangeinShoreHardnessShoreA,23°C,168hr,inWaterISO18175.0
Change in Ultimate Elongation23°C,168hr,inIRM903OilASTMD471-68%
Change in Ultimate Elongation23°C,168hr,inSodiumHydroxide,50%ASTMD471-7.0%
Change in Ultimate Elongation23°C,168hr,在水中ASTMD471-12%
Change in Ultimate Elongation23°C,168hr,inEthanol,95%ASTMD471-3.0%
Change in Ultimate Elongation23°C,168hr,inHydrochloricAcid,10%ASTMD471-9.0%
Elastomers PropertiesTest ConditionTest MethodTest ResultUnit
Compression Set125°C,70hrASTMD395B55%
Compression Set125°C,70hrISO81555%
Tensile Elongation(Across Flow)Break,23°CASTMD412600%
Tensile Elongation(Across Flow)Break,23°CISO37600%
hardnessTest ConditionTest MethodTest ResultUnit
Shore HardnessShore A,15sec,23°CISO86853
FlammabilityTest ConditionTest MethodTest ResultUnit
UL flame retardant rating1.1mmUL94HB
UL flame retardant rating2.9mmUL94HB
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.