TPU Elastollan® 1195A10 BASF GERMANY
191
- Unit Price:
- $4928 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 188MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Hydrolysis resistance Antibacterial High toughness
- Application Areas:Cable household electrical appl Fitness equipment
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt Mass-Flow Rate | 210°C/10.0kg | ASTMD1238 | 35to65 | g/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Taber Abrasion Resistance | ASTMD1044 | 55.0 | mg | |
Abrasion-DIN | DIN53516 | 25 | mm³ | |
Tensile Modulus | Injection | ASTMD412 | 51.7 | Mpa |
ASTM D-638 | 41.4 | Mpa | ||
Tensile Elongation | Break | ASTM D-412 | 450 | % |
Flexural Modulus | Injection | ASTMD790 | 52.4 | Mpa |
Tearing Strength | ASTM D-624 | 140 | kN/m | |
Tensile Strength(Break) | ASTM D-412 | 48.3 | Mpa | |
Tensile Stress (100%) | ASTM D-412 | 16.5 | Mpa | |
hardness | shoreA | ASTM D-648 | 95 |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Glass Transition Temperature | 内部方法 | -28.0 | °C | |
SofteningPoint DMA | 内部方法 | 89 | °C | |
Vicat Softening Temperature | ASTMD1525 | 127 | °C | |
Vicat Softening Temperature | ASTM D-1525 | 116 | °C |
Elastomers Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | 100%Strain | ASTMD412 | 17.2 | Mpa |
300%Strain | ASTMD412 | 35.9 | Mpa | |
Tensile Strength | ASTMD412 | 39.3 | Mpa | |
Tensile Elongation | Break | ASTMD412 | 430 | % |
Tearing Strength | ASTMD624 | 140 | kN/m | |
Compression Set | 23°C,22hr | ASTMD395B | 30 | % |
70°C,22hr | ASTMD395B | 45 | % |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore Hardness | Shore A | ASTMD2240 | 95 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.75mm | UL94 | HB | |
3.0mm | UL94 | HB |
Physical | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt index | ASTM D-1238 | 50 | g/10min | |
Density | ASTM D-792 | 1.14 | g/cm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.