ASA GELOY™ HRA222F-10000 SABIC INNOVATIVE SHANGHAI
162
- Unit Price:
- $4450 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 71MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High temperature resistan Thermal stability
- Application Areas:Lawn garden equipment Home appliance components
- Color:--
- Grade:Flame retardant grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Moisture Absorption | Saturation, 23°C | ISO 62 | 0.60 | % |
Equilibrium, 23°C, 50% RH | ISO 62 | 0.20 | % | |
Outdoor Suitability | UL 746C | f1 | ||
Melt Volume flow Rate | 260°C/2.16 kg | ISO 1133 | 13.0 | cm3/10min |
Modeling Shrinkage - Flow | 内部方法 | 0.40 到 0.60 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Modulus | ISO 178 | 2510 | Mpa | |
Flexural Stress | ISO 178 | 93.0 | Mpa | |
Tensile Modulus | -- 3 | ASTM D638 | 2590 | Mpa |
-- | ISO 527-2/1 | 2520 | Mpa | |
Tensile Elongation | Yield 5 | ASTM D638 | 4.2 | % |
Yield 4 | ASTM D638 | 4.3 | % | |
Yield | ISO 527-2/5 | 4.3 | % | |
Yield | ISO 527-2/50 | 4.4 | % | |
Break 5 | ASTM D638 | > 100 | % | |
Break 4 | ASTM D638 | > 100 | % | |
Break | ISO 527-2/5, ISO 527-2/50 | > 50 | % | |
Tensile Strength | Yield 4 | ASTM D638 | 63.0 | Mpa |
Yield 5 | ASTM D638 | 59.0 | Mpa | |
Yield | ISO 527-2/5 | 62.0 | Mpa | |
Yield | ISO 527-2/50 | 60.0 | Mpa | |
Break 5 | ASTM D638 | 66.0 | Mpa | |
Break 4 | ASTM D638 | 56.0 | Mpa | |
Break | ISO 527-2/5 | 51.0 | Mpa | |
Break | ISO 527-2/50 | 45.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Vicat Softening Temperature | -- | ISO 306/A50 | 111 | °C |
-- | ISO 306/B50 | 102 | °C | |
-- | ISO 306/B120 | 104 | °C | |
Ball PressureTest | 73 to 77°C | IEC 60695-10-2 | 通过 | |
Linear thermal expansion coefficient | Flow : -30 to 80°C | ISO 11359-2 | 6.9E-5 | cm/cm/°C |
Across Flow : -30 to 80°C | ISO 11359-2 | 7.1E-5 | cm/cm/°C | |
Across Flow : 23 to 80°C | ISO 11359-2 | 7.5E-5 | cm/cm/°C | |
RTI | UL 746 | 90.0 | °C | |
RTI Imp | UL 746 | 90.0 | °C | |
RTI Elec | UL 746 | 90.0 | °C | |
Heat Deflection Temperature | 0.45 MPa, Unannealed, 4.00 mm, 100 mm Span | ISO 75-2/Be | 99.0 | °C |
1.8 MPa, Unannealed, 4.00 mm, 100 mm Span | ISO 75-2/Ae | 88.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Comparative Tracking Index | UL 746 | PLC 0 | ||
Comparative Tracking Index | IEC 60112 | 600 | V |
Injection | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Drying Time | 2.0 到 4.0 | hr | ||
Rear Temperature | 200 到 230 | °C | ||
Middle Temperature | 220 到 260 | °C | ||
Front Temperature | 230 到 270 | °C | ||
Nozzle Temperature | 220 到 260 | °C | ||
Drying Temperature | 80 到 90 | °C | ||
Suggested Max Moisture | 0.020 | % | ||
Processing (Melt) Temp | 230 到 270 | °C | ||
Mold Temperature | 50 到 70 | °C | ||
Hopper Temperature | 60 到 80 | °C |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Oxygen Index | ISO 4589-2 | 29 | % | |
Flame Rating | 2.0 mm | UL 94 | V-0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.