Material Description
Technical Data Sheet
Material Description
- Material Properties:Chemical resistance High rigidity
- Application Areas:Household daily necessiti Household goods doors and windows
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Moisture Absorption | Saturation,23°C | ISO62 | 1.7 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.35 | % | |
Melt Volume flow Rate | 220°C/10.0kg | ISO1133 | 8.00 | cm3/10min |
Density / Specific Gravity | ISO1183 | 1.07 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Stress | ISO178 | 80.0 | Mpa | |
Tensile Creep Modulus | 1000hr | ISO899-1 | 1400 | Mpa |
Tensile Stress | Yield,23°C | ISO527-2 | 56.0 | Mpa |
Tensile Strain | Yield,23°C | ISO527-2 | 3.1 | % |
Tensile Modulus | ISO527-2 | 2600 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Linear thermal expansion coefficient | MD | ISO11359-2 | 8.0E-5到1.1E-4 | cm/cm/°C |
Vicat Softening Temperature | -- | ISO306/A50 | 105 | °C |
-- | ISO306/B50 | 98.0 | °C | |
Thermal Conductivity | DIN52612 | 0.17 | W/m/K | |
Heat Deflection Temperature | 0.45MPa,Annealed | ISO75-2/B | 101 | °C |
1.8MPa,Annealed | ISO75-2/A | 97.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface Resistivity | IEC60093 | 1E+13 | ohms | |
Dielectric Constant | 100Hz | IEC60250 | 3.70 | |
1.00mm,1MHz | IEC60250 | 3.40 | ||
Volume Resistivity | IEC60093 | 1E+14 | ohms·cm | |
Dissipation Factor? | 100Hz | IEC60250 | 9E-03 | |
1MHz | IEC60250 | 0.025 |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | -30°C | ISO179 | 3.0 | kJ/m² |
23°C | ISO179 | 12 | kJ/m² | |
Notched Izod Impact Strength | -30°C | ISO180/A | 3.0 | kJ/m² |
23°C | ISO180/A | 13 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Ball Indentation Hardness | ISO2039-1 | 100 | Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.