ASA Luran®S 757G BASF GERMANY
187
- Unit Price:
- $2416 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 55MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | ISO294-4 | 0.50to0.90 | % | |
Moisture Absorption | Saturation,23°C | ISO62 | 1.7 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.35 | % | |
Melt Volume flow Rate | 220°C/10.0kg | ISO1133 | 25.0 | cm3/10min |
Density / Specific Gravity | ISO1183 | 1.07 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Stress | ISO178 | 75.0 | Mpa | |
Tensile Creep Modulus | 1hr | ISO899-1 | 2200 | Mpa |
Tensile Stress | Yield,23°C | ISO527-2 | 51.0 | Mpa |
Tensile Strain | Yield,23°C | ISO527-2 | 3.3 | % |
Tensile Creep Modulus | 1000hr | ISO899-1 | 1650 | Mpa |
Tensile Modulus | ISO527-2 | 2400 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Vicat Softening Temperature | -- | ISO306/A50 | 105 | °C |
-- | ISO306/B50 | 97.0 | °C | |
Thermal Conductivity | DIN52612 | 0.17 | W/m/K | |
Heat Deflection Temperature | 0.45MPa,Annealed | ISO75-2/B | 101 | °C |
1.8MPa,Annealed | ISO75-2/A | 96.0 | °C | |
Linear thermal expansion coefficient | MD | ISO11359-2 | 8.0E-5to1.1E-4 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface Resistivity | IEC60093 | 1E+13 | ohms | |
Dielectric Constant | 100Hz | IEC60250 | 3.40 | |
Volume Resistivity | IEC60093 | 1E+14 | ohms·cm | |
Dissipation Factor? | 100Hz | IEC60250 | 0.010 | |
1MHz | IEC60250 | 0.025 |
Film | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Elongation - MD | Break | ISO527-3 | 8.0 | % |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | -30°C | ISO179 | 3.0 | kJ/m² |
23°C | ISO179 | 12 | kJ/m² | |
Notched Izod Impact Strength | -30°C | ISO180/A | 4.0 | kJ/m² |
23°C | ISO180/A | 11 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Ball Indentation Hardness | ISO2039-1 | 90.0 | Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.