Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage(Across Flow) | / | ISO 294-4, 2577 | 1 | % |
Modeling Shrinkage (Across Flow) | / | ISO 294-4, 2577 | 1 .3 | % |
Melt Mass-Flow Rate (380°C 5kg) | / | ISO 1133 | 10 | g/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Flexural Modulus | 23°C | ISO 178 | 4100 | Mpa |
Flexural Strength | 23°C | ISO 178 | 165 | Mpa |
Tensile Strength(Yield) | 50mm/m | ISO 527-2/1A | 100 | Mpa |
Tensile Elongation (Break) | 50mm/m | ISO 527-2/1A | 45 | % |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Notched Impact Strength | 23℃ (73℉) | ISO 179/1eA | 7 | kJ/m² |
Charpy Unnotched Impact Strength | 23℃ (73℉) | ISO 179/1eU | NB | |
Unnotched Izod Impact Strength | 23℃ (73℉) | ISO 180/1A | 7.5 | kJ/m² |
Unnotched Izod Impact Strength | 23℃ (73℉) | ISO 180/1U | NB | kJ/m² |
Electrical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Volume Resistivity | | IEC 60093 | 100000000000000 | Ohm-m |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Coefficient of Linear Thermal Expansion(Flow) | Above Tg | ISO 11359-2 | 120 E-6 | °C |
Coefficient of Linear Thermal Expansion(Flow) | Below Tg | ISO 11359-2 | 45 E-6 | °C |
Melt Temperature | -40°C to | ISO 11357-1/-3 | 343 | °C |
Glass Transition Temperature | -40°C to | ISO 11357-1/-2 | 143 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.