PEEK VESTAKEEP® 4000G EVONIK GERMANY
175
- Unit Price:
- $82845 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 36MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Semi crystalline Chemical resistance Self extinguishing high viscosity
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt Volume flow Rate | 380°C/5.0kg | ISO1133 | 11.0 | cm3/10min |
Density / Specific Gravity | ISO1183 | 1.30 | g/cm³ | |
Modeling Shrinkage | TD:180°C,2.00mm | ISO294-4 | 1.1 | % |
MD:180°C,2.00mm | ISO294-4 | 0.90 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Modulus | ISO527-2 | 3500 | Mpa | |
Tensile Stress | Yield | ISO527-2 | 96.0 | Mpa |
Tensile Strain | Yield | ISO527-2 | 5.0 | % |
Break | ISO527-2 | 30 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Vicat Softening Temperature | -- | ISO306/A | 335 | °C |
-- | ISO306/B | 305 | °C | |
Linear thermal expansion coefficient | MD:23to55°C | ISO11359-2 | 6E-04 | cm/cm/°C |
Melting Temperature | ISO3146 | 340 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Relative Permittivity | 50Hz | IEC60250 | 2.80 | |
1MHz | IEC60250 | 2.80 | ||
Comparative Tracking Index | SolutionA5 | IEC60112 | 175 | V |
SolutionA | IEC60112 | 200 | V | |
Dielectric Strength | IEC60243-1 | 16 | KV/mm | |
Surface Resistivity | IEC60093 | 1E+14 | ohms | |
Volume Resistivity | IEC60093 | 1E+15 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | NoBreak | |
23°C | ISO179/1eU | NoBreak | ||
Charpy Notched Impact Strength | -30°C,Complete Break | ISO179/1eA | 6.0 | kJ/m² |
23°C,Complete Break | ISO179/1eA | 7.0 | kJ/m² |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 3.2mm | UL94 | V-0 | |
Glow Wire Flammability Index | 2.0mm | IEC60695-2-12 | 960 | °C |
Glow Wire Ignition Temperature | 2.0mm | IEC60695-2-13 | 825 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.