PEEK KetaSpire® PEEK KT-820SL45 SOLVAY USA
92
- Unit Price:
- $85652 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 14MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:--
- Application Areas:Bushing Gear Application in the automo Oil/Gas Supplies Thrust washer
- Color:--
- Grade:--
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.18mm | ASTMD955 | 0.0到0.20 | % |
TD:3.18mm | ASTMD955 | 1.3到1.5 | % | |
Moisture Absorption | 24hr | ASTMD570 | 0.030 | % |
Melt Mass-Flow Rate | 400°C/2.16kg | ASTMD1238 | 2.0 | g/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | Yield | ISO527-2/1A/5 | 197 | Mpa |
-- | ASTMD638 | 161 | Mpa | |
Tensile Modulus | -- | ASTMD638 | 18300 | Mpa |
-- | ISO527-2/1A/1 | 25300 | Mpa | |
Tensile Elongation | Break3 | ASTMD638 | 1.5 | % |
Break | ISO527-2/1A/5 | 1.5 | % | |
Flexural Modulus | -- | ASTMD790 | 16600 | Mpa |
-- | ISO178 | 24100 | Mpa | |
Flexural Strength | -- | ASTMD790 | 265 | Mpa |
-- | ISO178 | 273 | Mpa | |
Compressive Strength | ASTMD695 | 127 | Mpa | |
Shearing Strength | ASTMD732 | 84.1 | Mpa | |
Coefficient of Friction | --4 | ASTMD1894 | 0.34 | |
--5 | ASTMD3702 | 0.45 | ||
--6 | ASTMD1894 | 0.12 | ||
--7 | ASTMD3702 | 0.070 |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Specific Heat | 50°C | DSC | 1250 | J/kg/°C |
200°C | DSC | 1670 | J/kg/°C | |
Thermal Conductivity | ASTME1530 | 0.36 | W/m/K | |
Deflection Temperature Under Load? | 1.8MPa,Annealed | ASTMD648 | 299 | °C |
Linear thermal expansion coefficient | MD:-50to50°C | ASTME831 | 1.7E-05 | cm/cm/°C |
Peak Melting Temperature | ASTMD3418 | 342 | °C | |
Glass Transition Temperature | ASTMD3418 | 152 | °C |
Fill Analysis | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt Viscosity | 400°C,1000sec^-1 | ASTMD3835 | 380 | Pa·s |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Unnotched Izod Impact Strength | -- | ASTMD4812 | 530 | J/m |
-- | ISO180 | 43 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | M-Scale | ASTMD785 | 90 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.