Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Moisture Absorption | Saturation,23°C | ISO62 | 0.20 | % |
Moisture Absorption | Equilibrium,23°C,50%RH | ISO62 | 0.64 | % |
Melt Volume flow Rate | 230°C/2.16kg | ISO1133 | 4.00 | cm3/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Modulus | | ISO527-2 | 45.0 | Mpa |
Tensile Stress | Break | ISO527-2 | 9.70 | Mpa |
Tensile Stress | 10%Strain | ISO527-2 | 2.60 | Mpa |
Tensile Stress | 100%Strain | ISO527-2 | 4.50 | Mpa |
Nominal Tensile Strain at Break | | ISO527-2 | 420 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Linear thermal expansion coefficient | MD | ISO11359-2 | 1.8E-04 | cm/cm/°C |
Linear thermal expansion coefficient | TD | ISO11359-2 | 1.9E-04 | cm/cm/°C |
Melting Temperature | | ISO11357-3 | 180 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Relative Permittivity | 100Hz | IEC60250 | 3.70 | |
Relative Permittivity | 1MHz | IEC60250 | 3.50 | |
Volume Resistivity | | IEC60093 | 8.3E+12 | ohms·cm |
Dielectric Strength | | IEC60243-1 | 20 | KV/mm |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Shore Hardness | Shore A,3sec | ISO868 | 88 | |
Shore Hardness | Shore D,3sec | ISO868 | 42 | |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 0.8mm | IEC60695-11-10,-20 | V-2 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.