PA612 Zytel® 77G33L NC010 DUPONT USA
164
- Unit Price:
- $4850 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:wear resistant High impact resistance
- Application Areas:Electrical tools electrical equipment Automotive Applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density | ASTM D792/ISO 1183 | 1.32 | ||
Modeling Shrinkage | ASTM D955 | 0.3~0.9 | % | |
Moisture Absorption 23℃/24H | ASTM D570/ISO 62 | 0.7 | % |
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.20mm | 0.20 | % | |
TD:3.20mm | 1.0 | % | ||
TD | ISO294-4 | 0.90 | % | |
MD | ISO294-4 | 0.30 | % | |
Moisture Absorption | 23°C,24hr | ISO62 | 0.30 | % |
Saturation,23°C,2.00mm | ISO62 | 1.8 | % | |
Equilibrium,23°C,2.00mm,50%RH | ISO62 | 0.70 | % | |
Ejection Temperature | 210 | °C | ||
SpecificHeatCapacityofMelt | 2130 | J/kg/°C | ||
ThermalConductivityofMelt | 0.26 | W/m/K | ||
Viscosity number | ISO307 | 100 | cm³/g |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Compressive Stress | ISO604 | 160 | Mpa | |
Shearing Strength | ASTMD732 | 75.0 | Mpa | |
Tensile Stress | Break | ISO527-2 | 170 | Mpa |
Tensile Strain | Break | ISO527-2 | 3.2 | % |
Flexural Stress | ISO178 | 260 | Mpa | |
Tensile Elongation?(Break) | ASTM D412/ISO 527 | 3.2 | % | |
Tensile Modulus | ASTM D412/ISO 527 | 9500 | kg/cm²(MPa)[Lb/in²] | |
ISO527-2 | 9500 | Mpa | ||
Tensile Strength | ASTM D412/ISO 527 | 168 | kg/cm²(MPa)[Lb/in²] | |
Flexural Modulus | ASTM D790/ISO 178 | 8200 | kg/cm²(MPa)[Lb/in²] | |
ISO178 | 8500 | Mpa | ||
Charpy impact strength | ASTM D256/ISO 179 | 13 | kg·cm/cm(J/M)ft·lb/in | |
ASTM D256/ISO 179 | 80 | kg·cm/cm(J/M)ft·lb/in | ||
ASTM D256/ISO 179 | 11 | kg·cm/cm(J/M)ft·lb/in | ||
ASTM D256/ISO 179 | 60 | kg·cm/cm(J/M)ft·lb/in |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Burning Rate | UL94 | HB | ||
Deflection Temperature Under Load? | ASTM D648/ISO 75 | 216 | ℃(℉) | |
ASTM D648/ISO 75 | 200 | ℃(℉) | ||
0.45MPa,Unannealed | ISO75-2/B | 216 | °C | |
1.8MPa,Unannealed | ISO75-2/A | 200 | °C | |
Melting Temperature | 218 | ℃(℉) | ||
Linear expansion coefficient | ASTM D696/ISO 11359 | 0.83~1.58 | ||
Linear thermal expansion coefficient | MD:-- | ISO11359-2 | 2E-05 | cm/cm/°C |
MD:-40to23°C | ISO11359-2 | 2.6E-05 | cm/cm/°C | |
MD:55to160°C | ISO11359-2 | 1.4E-05 | cm/cm/°C | |
TD:-- | ISO11359-2 | 1.1E-04 | cm/cm/°C | |
TD:-40to23°C | ISO11359-2 | 8.3E-05 | cm/cm/°C | |
TD:55to160°C | ISO11359-2 | 1.6E-04 | cm/cm/°C | |
TD:EffectiveThermalDiffusivity | ISO11359-2 | 7.5E-08 | m²/s | |
Melting Temperature | ISO11357-3 | 218 | °C | |
Glass Transition Temperature | ISO11357-2 | 65.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dissipation Factor? | 100Hz | IEC60250 | 0.014 | |
1MHz | IEC60250 | 0.020 | ||
Relative Permittivity | 100Hz | IEC60250 | 4.10 | |
1MHz | IEC60250 | 3.70 | ||
Comparative Tracking Index | IEC60112 | 600 | V | |
Dielectric Strength | IEC60243-1 | 33 | KV/mm | |
Surface Resistivity | ASTM D257/IEC 60093 | 1.00E+12 | Ω | |
Volume Resistivity | IEC60093 | 1E+15 | ohms·cm | |
ASTM D257/IEC 60093 | 1.00E+13 | Ω.cm | ||
Dielectric loss | ASTM D150/IEC 60250 | 4.1 |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Notched Izod impact strength | -30°C | ISO180/1U | 60 | kJ/m² |
23°C | ISO180/1U | 70 | kJ/m² | |
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | 60 | kJ/m² |
23°C | ISO179/1eU | 80 | kJ/m² |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.70mm | UL94 | HB | |
1.5mm | UL94 | HB | ||
0.70mm | IEC60695-11-10,-20 | HB | ||
1.5mm | IEC60695-11-10,-20 | HB | ||
Oxygen Index | ISO4589-2 | 23 | % | |
FMVSS Flammability | FMVSS302 | B | ||
Fogging-G-value | condensate | ISO6452 | 1E-04 | g |
Burning Rate | 1.00mm | ISO3795 | 23 | mm/min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.