Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Density | | ASTM D792/ISO 1183 | 1.01 | kg·cm/cm(J/M)ft·lb/in |
Moisture Absorption 23℃/24H | | ASTM D570/ISO 62 | 1.5 | % |
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | TD | ISO294-4 | 1.2 | % |
Modeling Shrinkage | MD | ISO294-4 | 0.85 | % |
Moisture Absorption | Saturation,23°C | ISO62 | 1.5 | % |
Moisture Absorption | Equilibrium,23°C,50%RH | ISO62 | 0.80 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Stress | Yield | ISO527-2 | 45.0 | Mpa |
Tensile Strain | Yield | ISO527-2 | 5.0 | % |
Tensile Strain | Break | ISO527-2 | >50 | % |
Tensile Elongation?(Break) | | ASTM D412/ISO 527 | >50 | % |
Tensile Modulus | | ASTM D412/ISO 527 | 1350 | kg/cm²(MPa)[Lb/in²] |
Tensile Modulus | | ISO527-2 | 1350 | Mpa |
Tensile Elongation | | ASTM D412/ISO 527 | 5 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | | ASTM D648/ISO 75 | 50 | ℃(℉) |
Deflection Temperature Under Load? | | ASTM D648/ISO 75 | 110 | ℃(℉) |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ISO75-2/A | 50.0 | °C |
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 110 | °C |
Melting Temperature | | | 178 | ℃(℉) |
Vicat Softening Temperature | -- | ISO306/A | 170 | °C |
Vicat Softening Temperature | -- | ISO306/B | 140 | °C |
Melting Temperature | | ISO11357-3 | 178 | °C |
Linear thermal expansion coefficient | MD:23to55°C | ISO11359-2 | 1.5E-04 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dielectric Strength | | IEC60243-1 | 27 | KV/mm |
Relative Permittivity | 23°C,100Hz | IEC60250 | 3.80 | |
Relative Permittivity | 23°C,1MHz | IEC60250 | 2.50 | |
Comparative Tracking Index | -- | IEC60112 | 600 | V |
Comparative Tracking Index | SolutionA3 | IEC60112 | >600 | V |
Dissipation Factor? | 23°C,1MHz | IEC60250 | 0.031 | |
Dissipation Factor? | 23°C,100Hz | IEC60250 | 0.045 | |
Volume Resistivity | | IEC60093 | 1E+15 | ohms·cm |
Volume Resistivity | | ASTM D257/IEC 60093 | 10^15 | Ω.cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | NoBreak | |
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | NoBreak | |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 1.6mm | UL94 | HB | |
UL flame retardant rating | 3.2mm | UL94 | HB | |
Supplementary information | Test Condition | Test Method | Test Result | Unit |
---|
ElectrolyticalCorrosion | | IEC60426 | A1 | |
ISO Shortname | | ISO1874 | PA12,KH,18-010 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.