Technical Data Sheet
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Strength(Yield) | ISO 527-2 | 28 | Mpa | |
Tensile Elongation (Break) | ISO 527-2 | 2.3 | % | |
Charpy Unnotched Impact Strength | +23℃/-30℃ | ISO 179/1eU | 100/30 | KJ/m |
Shore Hardness (A/D) | ISO 868 | D58 | ||
Charpy Notched Impact Strength | +23℃/-30℃ | ISO 179/1eA | 4/3 | KJ/m |
Elongation at break | ISO 527-2 | >50 | % | |
Flexural Modulus | ISO 527-2 | 1550 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL94 | 厚度3.2mm/1.6mm | UL 94 | HB/HB | CLASS |
Melt Temperature | 180-250 | °C | ||
Melt Temperature | 30-50 | °C | ||
Melt Temperature | 190-230 | °C | ||
Deflection Temperature Under Load? | 1.8MPa | ISO 75 | 55 | °C |
0.455MPa | ISO 75 | 75 | °C | |
Vicat Softening Temperature | ISO 306 | 59 | °C | |
A/120 | ISO 306 | 85 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric Constant | 10Hz-1MHz | IEC 250 | 2.5 | |
Surface resistance | IEC 243/1 | >10 | ||
Dielectric Strength | IEC 93 | 140 | KV/mm | |
Volume Resistivity | IEC 93 | >10 | Ω.cm |
Physical | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Moisture Absorption | 23℃,纯水中 | ISO 62 | 0.07 | % |
Melt Volume flow Rate | 200℃/5kg | ISO 1133 | 11 | CM |
Density / Specific Gravity | ISO 1183 | 1.01 | g/cm | |
Moisture Absorption | 23℃,50%湿度 | ISO 62 | 0.07 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.