Material Description
Technical Data Sheet
Material Description
- Material Properties:Food contact compliance
- Application Areas:film Pipe fittings
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Moisture Absorption | Saturation,23°C | ISO62 | 0.50 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.25 | % | |
Melt Volume flow Rate | 250°C/2.16kg | ISO1133 | 19.0 | cm3/10min |
parent Viscosity | 降低的粘度 | ISO1628 | 130.0 | ml/g |
Density / Specific Gravity | ISO1183 | 1.30 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Stress | 23°C | ISO178 | 85.0 | Mpa |
Nominal Tensile Strain at Break | 23°C | ISO527-2 | >50 | % |
Tensile Creep Modulus | 1000hr | ISO899-1 | 1200 | Mpa |
Tensile Stress | Yield,23°C | ISO527-2 | 55.0 | Mpa |
Tensile Strain | Yield,23°C | ISO527-2 | 3.7 | % |
Tensile Modulus | 23°C | ISO527-2 | 2500 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ISO75-2/A | 65.0 | °C |
0.45MPa,Unannealed | ISO75-2/B | 165 | °C | |
Melting temperature (DSC) | ISO3146 | 223 | °C | |
Linear thermal expansion coefficient | MD | 1.4E-04 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dissipation Factor? | 100Hz | IEC60250 | 1E-03 | |
1MHz | IEC60250 | 0.020 | ||
Surface Resistivity | IEC60093 | 1E+13 | ohms | |
Dielectric Constant | 100Hz | IEC60250 | 3.30 | |
1MHz | IEC60250 | 3.30 | ||
Volume Resistivity | IEC60093 | 1E+14 | ohms·cm | |
Comparative Tracking Index | IEC60112 | 550 | V |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO179 | 6.0 | kJ/m² |
Charpy Unnotched Impact Strength | 23°C | ISO179 | 290 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Ball Indentation Hardness | ISO2039-1 | 130 | Mpa |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 1.5mm | UL94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.