Need Help? Contact Us service@plas.com
Get App

PPO NORYL™  731S-111 SABIC INNOVATIVE SHANGHAI

220
  • Unit Price:
    $4918 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    34MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:High mobility Antistatic High temperature resistan currency
  • Application Areas:Food containers
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

physical property Test ConditionTest MethodTest ResultUnit
Water absorption rateSaturation, 23°CISO 620.23%
Water absorption rateEquilibrium, 23°C, 50% RHISO 620.060%
Molten Volume Flow Rate (MVR)280°C/5.0 kgISO 11338.00cm3/10min
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile stressYieldISO 527-2/5055.0Mpa
Tensile stressBreakISO 527-2/5050.0Mpa
Tensile strainYieldISO 527-2/505.0%
Tensile strainBreakISO 527-2/5030%
Tensile modulusISO 527-2/12300Mpa
Bending modulus 2ISO 1782200Mpa
Bending stress 2, 3ISO 17875.0Mpa
Thermal performanceTest ConditionTest MethodTest ResultUnit
Hot deformation temperature1.8 MPa, Unannealed, 4.00 mm, 100 mm SpanISO 75-2/Ae115°C
Vicat softening temperature--ISO 306/B50135°C
Vicat softening temperature--ISO 306/B120140°C
Linear coefficient of thermal expansionFlow : 23 to 80°CISO 11359-27.0E-5cm/cm/°C
Linear coefficient of thermal expansionAcross Flow : 23 to 80°CISO 11359-27.0E-5cm/cm/°C
injectionTest ConditionTest MethodTest ResultUnit
drying temperature100 到 120°C
Processing (melt) temperature280 到 300°C
Mold temperature80 到 120°C
drying time2.0 到 3.0hr
Temperature at the rear of the barrel240 到 260°C
Temperature in the middle of the barrel260 到 280°C
Temperature at the front of the material cylinder280 到 300°C
Spray nozzle temperature260 到 280°C
Hopper temperature60 到 80°C
Impact performanceTest ConditionTest MethodTest ResultUnit
Impact strength of simply supported beam gap 4-30°CISO 179/1eA5.0kJ/m²
Impact strength of simply supported beam gap 423°CISO 179/1eA15kJ/m²
Suspended wall beam gap impact strength 5-30°CISO 180/1A5.0kJ/m²
Suspended wall beam gap impact strength 523°CISO 180/1A15kJ/m²
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.