PPO NORYL™ 731S-701 SABIC INNOVATIVE SHANGHAI
200
- Unit Price:
- $4946 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 15MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High mobility Antistatic High temperature resistan currency
- Application Areas:Food containers
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 0.060 | % |
Saturation, 23°C | ISO 62 | 0.23 | % | |
Molten Volume Flow Rate (MVR) | 280°C/5.0 kg | ISO 1133 | 8.00 | cm3/10min |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile stress | Break | ISO 527-2/50 | 50.0 | Mpa |
Yield | ISO 527-2/50 | 55.0 | Mpa | |
Tensile strain | Break | ISO 527-2/50 | 30 | % |
Yield | ISO 527-2/50 | 5.0 | % | |
Tensile modulus | ISO 527-2/1 | 2300 | Mpa | |
Bending modulus 2 | ISO 178 | 2200 | Mpa | |
Bending stress 2, 3 | ISO 178 | 75.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.8 MPa, Unannealed, 4.00 mm, 100 mm Span | ISO 75-2/Ae | 115 | °C |
Vicat softening temperature | -- | ISO 306/B120 | 140 | °C |
-- | ISO 306/B50 | 135 | °C | |
Linear coefficient of thermal expansion | Across Flow : 23 to 80°C | ISO 11359-2 | 7.0E-5 | cm/cm/°C |
Flow : 23 to 80°C | ISO 11359-2 | 7.0E-5 | cm/cm/°C |
injection | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
drying temperature | 100 到 120 | °C | ||
Processing (melt) temperature | 280 到 300 | °C | ||
Mold temperature | 80 到 120 | °C | ||
drying time | 2.0 到 3.0 | hr | ||
Temperature at the rear of the barrel | 240 到 260 | °C | ||
Temperature in the middle of the barrel | 260 到 280 | °C | ||
Temperature at the front of the material cylinder | 280 到 300 | °C | ||
Spray nozzle temperature | 260 到 280 | °C | ||
Hopper temperature | 60 到 80 | °C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Impact strength of simply supported beam gap 4 | 23°C | ISO 179/1eA | 15 | kJ/m² |
-30°C | ISO 179/1eA | 5.0 | kJ/m² | |
Suspended wall beam gap impact strength 5 | 23°C | ISO 180/1A | 15 | kJ/m² |
-30°C | ISO 180/1A | 5.0 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.