Need Help? Contact Us service@plas.com
Get App

PPO NORYL™  N1150 BK SABIC INNOVATIVE US

84
  • Unit Price:
    $3407 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    11MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Conductive
  • Application Areas:electromagnetic shielding
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Modeling ShrinkageMD:3.20mm内部方法0.50to0.70%
Moisture AbsorptionSaturation,23°CISO620.070%
Melt Mass-Flow Rate280°C/5.0kgASTMD123815g/10min
Melt Volume flow Rate280°C/5.0kgISO113315.0cm3/10min
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Tensile ElongationYieldASTMD6384.0%
Tensile ModulusASTMD6382700Mpa
Tensile StrengthBreakASTMD63855.0Mpa
Tensile StrengthYieldASTMD63875.0Mpa
Flexural Modulus50.0mmSpanASTMD7903050Mpa
Flexural StrengthYield,50.0mmSpanASTMD790117Mpa
Tensile StressYieldISO527-2/5072.0Mpa
Tensile StressBreakISO527-2/5052.0Mpa
Tensile StrainYieldISO527-2/503.5%
Tensile StrainBreakISO527-2/507.0%
Tensile ModulusISO527-2/12650Mpa
Flexural StrengthISO178105Mpa
Tensile ElongationBreakASTMD6388.0%
Flexural ModulusISO1782600Mpa
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Heat Deflection Temperature1.8MPa,Unannealed,64.0mmSpanISO75-2/Af109°C
Deflection Temperature Under Load?1.8MPa,Unannealed,3.20mmASTMD648108°C
Vicat Softening TemperatureASTMD152510130°C
Vicat Softening Temperature--ISO306/B50130°C
Vicat Softening Temperature--ISO306/B120132°C
Linear thermal expansion coefficientMD:-40to40°CASTME8315.5E-05cm/cm/°C
Linear thermal expansion coefficientMD:-40to40°CISO11359-25.5E-05cm/cm/°C
Linear thermal expansion coefficientTD:-40to40°CASTME8315.8E-05cm/cm/°C
Linear thermal expansion coefficientTD:-40to40°CISO11359-25.8E-05cm/cm/°C
Impact PropertiesTest ConditionTest MethodTest ResultUnit
Instrumented Dart Impact23°C,TotalEnergyASTMD376340.0J
Charpy Notched Impact Strength23°CISO179/1eA6.0kJ/m²
Notched Izod Impact Strength23°CISO180/1A6.0kJ/m²
Notched Izod Impact Strength-30°CISO180/1A4.0kJ/m²
FlammabilityTest ConditionTest MethodTest ResultUnit
Flame Rating0.75mmUL94V-0
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.