PPO NORYL™ N225X-111 SABIC INNOVATIVE US
84
- Unit Price:
- $3384 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 12MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Processability Chlorine resistance Bromine free Flame retardant Non brominated Improved processability a Non chlorinated Flame retardant Non brominated Improved processability a Non chlorinated Flame retardant
- Application Areas:medical care
- Color:--
- Grade:Flame retardant grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density | ASTM D-792 | 1.11 | ||
Modeling Shrinkage | ASTM D-955 | 5-7 | in/in E-3 | |
Modeling Shrinkage | ASTM D-955 | 5-7 | in/in E-3 |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Instrumented Dart Impact (-30℃) | ASTM D-3763 | 8.6 | ft-lbs | |
Reverse Notched Impact Strength | ASTM D-256 | 12.0 | ft-lb/in | |
Flexural Strength (Yield) | ASTM D-790 | 14400 | psi | |
Notched Izod Impact Strength | ASTM D-256 | 1.8 | ft-lb/in | |
Tensile Elongation (Yield) | ASTM D-638 | 8.0 | % | |
Reverse Notched Izod Impact Strength (23℃) | ASTM D 256 | 16.6 | ft-lb/in | |
Instrumented Dart Impact (23℃) | ASTM D-3763 | 29.0 | ft-lbs | |
Tensile Strength (Break) | ASTM D 638 | 7200 | psi | |
Notched Izod Impact Strength (23℃) | ASTM D-256 | 3.5 | ft-lb/in | |
Tensile Elongation (Break) | ASTM D-638 | 17.0 | % | |
Tensile Strength | ASTM D-638 | 9700 | psi | |
Tensile Modulus | ASTM D-790 | 361500 | psi |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Heat Deflection Temperature | ASTM D-648 | 211 | deg F | |
UL | E121562 | |||
Heat Deflection Temperature | UL 746B | 95 | deg C | |
Heat Deflection Temperature | UL 746B | 80 | deg C | |
Heat Deflection Temperature | ASTM D-648 | 229 | deg F | |
V-0 Rating | 测试厚度 | UL 94 | 0.060 | inch |
Vicat Softening Temperature | ASTM D-1525 | 264 | deg F | |
5VA Rating | 测试厚度 | UL 94 | 0.120 | inch |
Hot-wire Ignition | UL 746B | 95 | deg C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface Resistivity | ASTM D-257 | >1 E14 | ohm/sq | |
Volume Resistivity | ASTM D-257 | 2E+16 | ohm-cm | |
Dissipation Factor (50Hz) | ASTM D-150 | 0.0100 | ||
Dielectric Constant (50Hz) | ASTM D-150 | 2.69 | ||
Dissipation Factor (1 MHz) | ASTM D-150 | 0.0070 | ||
Dielectric Constant (1 MHz) | ASTM D-150 | 2.55 | ||
Dielectric Strength | ASTM D-149 | 414 | v/mil |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.