PPS Xytron™ Polyphenylene Sulphide G4010E BK001 DSM HOLAND
73
- Unit Price:
- $5281 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | Across Flow | ISO 294-4 | 0.50 | % |
流量 | ISO 294-4 | 0.20 | % | |
Moisture Absorption | Saturation, 23°C | ISO 62 | 0.020 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | Break | ISO 527-2 | 160 | Mpa |
Break, 120°C | ISO 527-2 | 65.0 | Mpa | |
Break, 160°C | ISO 527-2 | 50.0 | Mpa | |
Break, 200°C | ISO 527-2 | 40.0 | Mpa | |
Tensile Strain | Break | ISO 527-2 | 2.4 | % |
Break, 120°C | ISO 527-2 | 3.9 | % | |
Break, 160°C | ISO 527-2 | 4.4 | % | |
Break, 200°C | ISO 527-2 | 4.5 | % | |
Tensile Modulus | -- | ISO 527-2 | 12000 | Mpa |
120°C | ISO 527-2 | 6100 | Mpa | |
160°C | ISO 527-2 | 3900 | Mpa | |
200°C | ISO 527-2 | 3000 | Mpa | |
Flexural Modulus | -- | ISO 178 | 10000 | Mpa |
120°C | ISO 178 | 8500 | Mpa | |
160°C | ISO 178 | 4600 | Mpa | |
200°C | ISO 178 | 3100 | Mpa | |
Flexural Stress | ISO 178 | 230 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Linear thermal expansion coefficient | Flow 3 | ISO 11359-2 | 1.1E-5 | cm/cm/°C |
Flow | ISO 11359-2 | 1.5E-5 | cm/cm/°C | |
Across Flow | ISO 11359-2 | 5.5E-5 | cm/cm/°C | |
Across Flow 3 | ISO 11359-2 | 1.1E-4 | cm/cm/°C | |
Melting Temperature | ISO 11357-3 | 280 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dissipation Factor? | 5.00 GHz | IEC 60250 | 5.5E-3 | |
Dielectric Strength | IEC 60243-1 | 33 | KV/mm | |
Relative Permittivity | 5.00 GHz | IEC 60250 | 3.80 | |
Comparative Tracking Index | IEC 60112 | 175 | V | |
Volume Resistivity | IEC 60093 | > 1.0E+15 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | -30°C | ISO 179/1eU | 65 | kJ/m² |
23°C | ISO 179/1eU | 55 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.