Technical Data Sheet
Compare
Physical properties | Test Condition | Test Method | Test Result | Unit |
---|
density | | ASTM D792/ISO 1183 | 1.66 | |
Molding shrinkage rate | | ASTM D955 | 0.36 | % |
Water absorption rate 23 ℃/24h | | ASTM D570/ISO 62 | 0.02 | % |
physical property | Test Condition | Test Method | Test Result | Unit |
---|
Mold shrinkage rate | Across Flow | TORAY | 0.70 | % |
Taber abrasion | | ASTM D-D1044 | 50 | mg/1000次 |
Friction coefficient/against iron | | ASTM D-1894 | 0.25 | |
Limit PV value | | TORAY | 815 | KJ/m |
Mold shrinkage rate | Flow | TORAY | 0.20 | % |
Shrinkage rate | TD:3.00mm2 | 内部方法 | 0.80 | % |
Shrinkage rate | MD:3.00mm4 | 内部方法 | 0.20 | % |
Water absorption rate | 23°C,24hr | ISO62 | 0.020 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Tensile stress | Yield,23°C | ISO527-2 | 200 | Mpa |
Tensile strain | Break,23°C | ISO527-2 | 1.8 | % |
Bending modulus | 23°C | ISO178 | 15500 | Mpa |
Bending stress | 23°C | ISO178 | 305 | Mpa |
shear strength | 23°C | JISK7214 | 80.0 | Mpa |
Friction coefficient 4 | | | 0.25 | |
Taber abraser | 1000Cycles | ISO9352 | 50.0 | mg |
Elongation rate | 23℃ | ASTM D-638 | 3.6 | % |
elongation at break | | ASTM D638/ISO 527 | 1.8 | % |
tensile strength | | ASTM D638/ISO 527 | 200 | kg/cm²(MPa)[Lb/in²] |
Rockwell hardness | | ASTM D785 | 122 | |
Bending modulus | | ASTM D790/ISO 178 | 15.5 | kg/cm²(MPa)[Lb/in²] |
bending strength | | ASTM D790/ISO 178 | 305 | kg/cm²(MPa)[Lb/in²] |
Bending modulus | 23℃ | ASTM D-790 | 13.3 | GPa |
tensile strength | 23℃ | ASTM D-638 | 207 | Mpa |
bending strength | 23℃ | ASTM D-790 | 275 | Mpa |
Rockwell hardness | | ASTM D-785 | 122 | R |
compressive strength | | ASTM D-732 | 80 | |
Charpy impact strength | | ASTM D256/ISO 179 | 11 | kg·cm/cm(J/M)ft·lb/in |
Charpy impact strength | | ASTM D256/ISO 179 | 55 | kg·cm/cm(J/M)ft·lb/in |
IZOD impact strength | Notched | ASTM D-256 | 130 | J/m |
IZOD impact strength | Unnotched | ASTM D-256 | 55 | KJ/m |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Combustibility (rate) | | UL94 | V-0 | |
Hot deformation temperature | | ASTM D648/ISO 75 | >260 | ℃(℉) |
melting point | | | 278 | ℃(℉) |
Hot deformation temperature | 1.82MPa | ASTM D-648 | >260 | °C |
Thermal expansion coefficient | Flow | ASTM D-696 | 2.3 | |
Thermal expansion coefficient | Across Flow | ASTM D-696 | 3.2 | |
melting point | | DSC | 278 | °C |
Hot deformation temperature | 1.8MPa,Unannealed | ISO75-2/A | 260 | °C |
Melting temperature | | ISO11357-3 | 278 | °C |
Linear coefficient of thermal expansion | MD | ISO11359-2 | 2.3E-05 | cm/cm/°C |
Linear coefficient of thermal expansion | TD | ISO11359-2 | 3.1E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Volume resistivity | | IEC60093 | 1E+16 | ohms·cm |
Dielectric strength | | IEC60243-1 | 24 | KV/mm |
Dielectric constant 6 | 23°C,1MHz | IEC60250 | 4.20 | |
Dissipation factor 5 | 23°C,1MHz | IEC60250 | 2E-03 | |
Dielectric constant | | ASTM D150/IEC 60250 | 4.2 | |
Volume resistivity | | ASTM D257/IEC 60093 | 1014 | Ω.cm |
Dielectric constant | 10 | ASTM D-150 | 3.8 | |
Volume resistance | | ASTM D-257 | 10 | Ω.m |
Arc resistance | | ASTM D-495 | 127 | |
loss factor | 10 | ASTM D-150 | 0.002 | |
Dielectric strength | | ASTM D-149 | 21 | MV/m |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|
Impact strength of simply supported beam without notch | 23°C | ISO179 | 55 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell hardness | R-Scale | ISO2039-2 | 122 | |
flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 0.28mm | UL94 | V-0 | |
Basic performance | Test Condition | Test Method | Test Result | Unit |
---|
Water absorption rate | 24hr,23℃于水中 | ASTM D-570 | 0.02 | % |
Supplementary Information | Test Condition | Test Method | Test Result | Unit |
---|
BarFlowLength6 | 320°C,1.00mm | 内部方法 | 135 | mm |
Other performance | Test Condition | Test Method | Test Result | Unit |
---|
Flowing Long | 320℃,98MPa | TORAY | 100 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.