- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Material Certification
Technical Data Sheet
Material Description
- Material Properties:Low warpage|Easy to process|Flame retardant|Glass fiber reinforced|Filler: Long glass fiber
- Application Areas:Household appliances|Spool|Laptop case
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Modeling Shrinkage | TD | 内部方法 | 0.63 % |
Moisture Absorption | 饱和 | ASTMD570 | 0.020 % |
Modeling Shrinkage | MD | 内部方法 | 0.11 % |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat Deflection Temperature | 1.8MPa,未退火 | ASTMD648 | 270 °C |
Linear thermal expansion coefficient | MD:150°C | 内部方法 | 1E-05 cm/cm/°C |
TD:150°C | 内部方法 | 6.3E-05 cm/cm/°C | |
Thermal Conductivity | JISR2618 | 0.56 W/m/K |
Additional | Test Condition | Test Method | Test Result |
---|---|---|---|
Soldering | 内部方法 | 295 °C |
Flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Flame Rating | 0.30mm,Allcolors | UL94 | V-0 |
Oxygen Index | ISO 489 | 45 % |
Electrical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Dissipation Factor? | 1kHz | ASTMD150 | 0.024 |
1MHz | ASTMD150 | 0.030 | |
Arc Resistance | ASTMD495 | 180 sec | |
Comparative Tracking Index | IEC60112 | 150 V | |
Volume Resistivity | ASTMD257 | 1E+15 ohms·cm | |
Dielectric Constant | 1kHz | ASTMD150 | 4.70 |
1MHz | ASTMD150 | 4.10 |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Poisson Ratio | 7.58 | 0.41 | |
Tensile Strength | 屈服 | ASTMD638 | 134 Mpa |
Tensile Elongation | 断裂 | ASTMD638 | 4.5 % |
Flexural Modulus | 23°C | ASTMD790 | 12100 Mpa |
200°C | ASTMD790 | 4500 Mpa | |
Flexural Strength | 屈服,23°C | ASTMD790 | 145 Mpa |
屈服,200°C | ASTMD790 | 29.0 Mpa | |
Shearing Strength | ASTMD732 | 53.0 Mpa |
Hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell Hardness | R级 | ASTMD785 | 101 |
Impact Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Unnotched Izod Impact Strength | 6.40mm | ASTMD256 | 340 J/m |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.