LCP SUMIKASUPER® E6807LHF NC SUMITOMO JAPAN
247
Unit Price:$8152 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 78.2MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Low warpage Flame retardant Processability Glass fiber reinforced Filler: Long glass fiber
- Application Areas:Household appliances Household appliances Laptop case Spool
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD | 内部方法 | 0.11 | % |
TD | 内部方法 | 0.63 | % | |
Water absorption rate | Saturation | ASTMD570 | 0.020 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
elongation | Break | ASTMD638 | 4.5 | % |
Bending modulus | 23°C | ASTMD790 | 12100 | Mpa |
200°C | ASTMD790 | 4500 | Mpa | |
bending strength | Yield,23°C | ASTMD790 | 145 | Mpa |
Yield,200°C | ASTMD790 | 29.0 | Mpa | |
shear strength | ASTMD732 | 53.0 | Mpa | |
Poisson's ratio | 7.58 | 0.41 | ||
Tensile strength | Yield | ASTMD638 | 134 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
thermal conductivity | JISR2618 | 0.56 | W/m/K | |
Hot deformation temperature | 1.8MPa,Unannealed | ASTMD648 | 270 | °C |
Linear coefficient of thermal expansion | MD:150°C | 内部方法 | 1E-05 | cm/cm/°C |
TD:150°C | 内部方法 | 6.3E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Leakage Trace Index | IEC60112 | 150 | V | |
Dissipation factor | 1kHz | ASTMD150 | 0.024 | |
1MHz | ASTMD150 | 0.030 | ||
Dielectric constant | 1kHz | ASTMD150 | 4.70 | |
1MHz | ASTMD150 | 4.10 | ||
Arc resistance | ASTMD495 | 180 | sec | |
Volume resistivity | ASTMD257 | 1E+15 | ohms·cm |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Cantilever beam without notch impact strength | 6.40mm | ASTMD256 | 340 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | R-Scale | ASTMD785 | 101 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.30mm,Allcolors | UL94 | V-0 | |
Extreme Oxygen Index | ISO 489 | 45 | % |
Supplementary Information | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Soldering | 内部方法 | 295 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.