PC/ABS CYCOLOY™ MC8002-701 SABIC INNOVATIVE NANSHA
136
- Unit Price:
- $4387 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 70MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:heat-resisting
- Application Areas:Electrical field Electronic field Home appliance components Automotive sector Application in the automo
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:3.20mm | 内部方法 | 0.50to0.70 | % |
Water absorption rate | 24hr | ASTMD570 | 0.10 | % |
Equilibrium,23°C | ASTMD570 | 0.40 | % | |
Melt mass flow rate | 260°C/5.0kg | ASTMD1238 | 9.0 | g/10min |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Elongation rate 3 | Yield | ASTMD638 | 5.0 | % |
Tensile modulus 2 | ASTMD638 | 2210 | Mpa | |
Tensile strength 3 | Yield | ASTMD638 | 56.5 | Mpa |
Bending modulus 4 | 50.0mmSpan | ASTMD790 | 2340 | Mpa |
Bending strength 4 | Yield,50.0mmSpan | ASTMD790 | 86.2 | Mpa |
Elongation rate 4 | Break | ASTMD638 | 150 | % |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
thermal conductivity | ASTMC177 | 0.20 | W/m/K | |
Hot deformation temperature | 0.45MPa,Unannealed,3.20mm | ASTMD648 | 124 | °C |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 107 | °C | |
1.8MPa,Unannealed,6.40mm | ASTMD648 | 110 | °C | |
Linear coefficient of thermal expansion | MD:-40to40°C | ASTME831 | 7.2E-05 | cm/cm/°C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dart impact equipped with measuring instruments | -30°C,TotalEnergy | ASTMD3763 | 54.2 | J |
23°C,TotalEnergy | ASTMD3763 | 61.0 | J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.